ISO-LEN® 1000 has been proven for many years in various fields of application. Due to its wide range of characteristics, this all-round material is being used in products in all areas of technology where particularly high demands on material are required. By adding additives, we also deliver PE-UHMW finished parts with antistatic properties (ISO-LEN® 1000 AST). The key features are:


  • High abrasion resistance
  • Low friction coefficient
  • Self-lubricating
  • Very high notched impact strength
  • Related Standards

    This material data has been provided by ISO-TECH Kunststoff GmbH.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyValueComment

    Coefficient of friction

    0.12 [-]

    Show Supplier Material materials with Coefficient of friction of 0.12 [-]

    DIN 53375, A, Against dry running steel

    Density

    0.96 g/cm³

    Show Supplier Material materials with Density of 0.96 g/cm³

    max., ISO 1183

    Water absorption

    0.01 %

    Show Supplier Material materials with Water absorption of 0.01 %

    max.

    Mechanical

    PropertyValueComment

    Elastic modulus

    0.7 GPa

    Show Supplier Material materials with Elastic modulus of 0.7 GPa

    min., ISO 527

    Elongation

    200 %

    Show Supplier Material materials with Elongation of 200 %

    min., ISO 527

    Hardness, Ball Indentation

    30 MPa

    Show Supplier Material materials with Hardness, Ball Indentation of 30 MPa

    min., ISO 2039-1

    Hardness, Shore D

    61 [-]

    Show Supplier Material materials with Hardness, Shore D of 61 [-]

    ISO 868

    65 [-]

    Show Supplier Material materials with Hardness, Shore D of 65 [-]

    ISO 868

    Impact strength, Charpy notched

    80 kJ/m²

    Show Supplier Material materials with Impact strength, Charpy notched of 80 kJ/m²

    min., ISO 179

    Yield strength

    20 MPa

    Show Supplier Material materials with Yield strength of 20 MPa

    ISO 527

    Thermal

    PropertyValueComment

    Max service temperature

    80 °C

    Show Supplier Material materials with Max service temperature of 80 °C

    Longterm

    Long

    Short

    Melting point

    130 - 135 °C

    Show Supplier Material materials with Melting point of 130 - 135 °C

    ISO 3146

    Thermal conductivity

    0.41 W/(m·K)

    Show Supplier Material materials with Thermal conductivity of 0.41 W/(m·K)

    DIN 52612

    Flammability

    HB UL 94

    Electrical

    PropertyValueComment

    Surface resistivity

    1e+09 Ω/sq

    Show Supplier Material materials with Surface resistivity of 1e+09 Ω/sq

    max., IEC 60243

    Volume resistivity

    1e+06 Ω·cm

    Show Supplier Material materials with Volume resistivity of 1e+06 Ω·cm

    max., IEC 60243

    Technological properties

    Property
    Application areas

    Sliding parts, chain guidance and sliding profiles

    Certifications

    Food Contact: FDA, RoHS,REACH

    UV resistance

    Partly