Description

ISO-PP is often used in chemical plants thanks to its pronounced chemical resistance. This semi-crystalline thermoplastic also has a very low moisture absorption. The key features are:


  • Very high chemical resistance
  • Minimal moisture absorption
  • High dimensional stability
  • This material data has been provided by ISO-TECH Kunststoff GmbH.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyValueComment

    Density

    0.91 g/cm³

    Show Supplier Material materials with Density of 0.91 g/cm³

    ISO 1183

    Water absorption

    0.01 %

    Show Supplier Material materials with Water absorption of 0.01 %

    ISO 62

    Mechanical

    PropertyValueComment

    Elastic modulus

    1 GPa

    Show Supplier Material materials with Elastic modulus of 1 GPa

    ISO 527

    Elongation

    50 %

    Show Supplier Material materials with Elongation of 50 %

    min., ISO 527

    Elongation at yield

    10 %

    Show Supplier Material materials with Elongation at yield of 10 %

    ISO 527

    Hardness, Ball Indentation

    67 MPa

    Show Supplier Material materials with Hardness, Ball Indentation of 67 MPa

    ISO 2039-1

    Hardness, Shore D

    70 [-]

    Show Supplier Material materials with Hardness, Shore D of 70 [-]

    DIN 53505

    Impact strength, Charpy notched

    50 kJ/m²

    Show Supplier Material materials with Impact strength, Charpy notched of 50 kJ/m²

    ISO 179

    Yield strength

    30 MPa

    Show Supplier Material materials with Yield strength of 30 MPa

    ISO 527

    Impact strength, Charpy unnotched

    No break, ISO 179

    Thermal

    PropertyValuePressureComment

    Heat deflection temperature

    96 °C

    Show Supplier Material materials with Heat deflection temperature of 96 °C

    0.45 MPa

    Max service temperature

    100 °C

    Show Supplier Material materials with Max service temperature of 100 °C

    Longterm

    Long

    Short

    Min service temperature

    5 °C

    Show Supplier Material materials with Min service temperature of 5 °C

    Longterm

    Vicat softening temperature

    91 °C

    Show Supplier Material materials with Vicat softening temperature of 91 °C

    ISO 306, VST B50

    Flammability

    HB UL 94

    Electrical

    PropertyValueComment

    Dielectric constant

    2.3 [-]

    Show Supplier Material materials with Dielectric constant of 2.3 [-]

    DIN 53483

    Loss tangent

    0.0002 [-]

    Show Supplier Material materials with Loss tangent of 0.0002 [-]

    DIN 53483

    Volume resistivity

    1e+16 Ω·cm

    Show Supplier Material materials with Volume resistivity of 1e+16 Ω·cm

    min., VDE 0303

    Technological properties

    Property
    Certifications

    RoHS,REACH

    UV resistance

    Partly