PET ISO-TECH

Alternative and trade names
ISO-PET
Want to keep this datasheet? Save it now in your required format

Description

ISO-PET is a thermoplastic material that impresses with its hardness and an excellent sliding behaviour. ISO-PET is, for example, used in the food industry for guides, rollers or stops as well as in mechanical engineering as the basis for gears or slide elements. The key features are:


  • Very hard
  • Low cold flow
  • Excellent sliding behaviour
  • Related Standards

    This material data has been provided by ISO-TECH Kunststoff GmbH.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyTemperatureValueComment

    Coefficient of friction

    0.3 [-]

    Show Supplier Material materials with Coefficient of friction of 0.3 [-]

    DIN 53375, C, Against dry running steel

    Density

    23.0 °C

    1.39 g/cm³

    Show Supplier Material materials with Density of 1.39 g/cm³

    ISO 1183

    Water absorption

    23.0 °C

    0.25 %

    Show Supplier Material materials with Water absorption of 0.25 %

    ISO 62

    Mechanical

    PropertyTemperatureValueComment

    Elastic modulus

    23.0 °C

    3.5 GPa

    Show Supplier Material materials with Elastic modulus of 3.5 GPa

    ISO 527

    Elongation

    23.0 °C

    15 %

    Show Supplier Material materials with Elongation of 15 %

    ISO 527

    Elongation at yield

    23.0 °C

    4 %

    Show Supplier Material materials with Elongation at yield of 4 %

    ISO 527

    Hardness, Ball Indentation

    23.0 °C

    170 MPa

    Show Supplier Material materials with Hardness, Ball Indentation of 170 MPa

    ISO 2039-1

    Hardness, Rockwell R

    23.0 °C

    96 [-]

    Show Supplier Material materials with Hardness, Rockwell R of 96 [-]

    ISO 2039-1

    Hardness, Shore D

    23.0 °C

    84 [-]

    Show Supplier Material materials with Hardness, Shore D of 84 [-]

    DIN 53505

    Impact strength, Charpy notched

    23.0 °C

    2 kJ/m²

    Show Supplier Material materials with Impact strength, Charpy notched of 2 kJ/m²

    ISO 179

    Impact strength, Charpy unnotched

    23.0 °C

    50 kJ/m²

    Show Supplier Material materials with Impact strength, Charpy unnotched of 50 kJ/m²

    min., ISO 179

    Yield strength

    23.0 °C

    90 MPa

    Show Supplier Material materials with Yield strength of 90 MPa

    ISO 527

    Thermal

    PropertyTemperatureValueComment

    Coefficient of thermal expansion

    23.0 °C

    8E-5 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 8E-5 1/K

    DIN 53752

    Heat deflection temperature, 1.80 MPa

    80 °C

    Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 80 °C

    Max service temperature

    100 °C

    Show Supplier Material materials with Max service temperature of 100 °C

    Longterm

    Min service temperature

    -20 °C

    Show Supplier Material materials with Min service temperature of -20 °C

    Longterm

    Thermal conductivity

    23.0 °C

    0.29 W/(m·K)

    Show Supplier Material materials with Thermal conductivity of 0.29 W/(m·K)

    DIN 52612

    Flammability

    HB UL 94

    Electrical

    PropertyTemperatureValueComment

    Comparative tracking index

    23.0 °C

    600 V

    Show Supplier Material materials with Comparative tracking index of 600 V

    IEC 60112

    Dielectric constant, 1MHz

    23.0 °C

    3.2 [-]

    Show Supplier Material materials with Dielectric constant, 1MHz of 3.2 [-]

    DIN 53483

    Dielectric strength

    23.0 °C

    22 kV/mm

    Show Supplier Material materials with Dielectric strength of 22 kV/mm

    VDE 0303

    Loss tangent, 1MHz

    23.0 °C

    0.01 [-]

    Show Supplier Material materials with Loss tangent, 1MHz of 0.01 [-]

    DIN 53483

    Surface resistivity

    23.0 °C

    1.00E+13 Ω/sq

    Show Supplier Material materials with Surface resistivity of 1.00E+13 Ω/sq

    min., VDE 0303

    Volume resistivity

    23.0 °C

    1.00E+14 Ω·cm

    Show Supplier Material materials with Volume resistivity of 1.00E+14 Ω·cm

    min., VDE 0303

    Technological properties

    Property
    Application areas

    Sliding parts and rollers

    Certifications

    RoHS,REACH