Properties

General

PropertyValueComment

Density

1.03 g/cm³

Show Supplier Material materials with Density of 1.03 g/cm³

ISO 1183

Water absorption

1.1 %

Show Supplier Material materials with Water absorption of 1.1 %

ISO 62

Mechanical

PropertyValueComment

Elongation

10 %

Show Supplier Material materials with Elongation of 10 %

ISO 527

Flexural strength

90 MPa

Show Supplier Material materials with Flexural strength of 90 MPa

DIN 53452

Hardness, Ball Indentation

106 MPa

Show Supplier Material materials with Hardness, Ball Indentation of 106 MPa

DIN 53452

Hardness, Shore D

78 [-]

Show Supplier Material materials with Hardness, Shore D of 78 [-]

DIN 53505

Impact strength, Charpy notched

8 - 12 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 8 - 12 kJ/m²

ISO 179

Impact strength, Charpy unnotched

110 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 110 kJ/m²

ISO 179

Tear strength

No break, ISO 527

Thermal

PropertyValuePressureComment

Coefficient of thermal expansion

8e-05 - 0.0001 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 8e-05 - 0.0001 1/K

DIN 52328

Heat deflection temperature

185 °C

Show Supplier Material materials with Heat deflection temperature of 185 °C

0.45 MPa

190 °C

Show Supplier Material materials with Heat deflection temperature of 190 °C

0.45 MPa

Max service temperature

120 °C

Show Supplier Material materials with Max service temperature of 120 °C

Longterm

Long

Short

Min service temperature

-50 °C

Show Supplier Material materials with Min service temperature of -50 °C

Longterm

Thermal conductivity

0.23 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 0.23 W/(m·K)

DIN 52612

Vicat softening temperature

182 °C

Show Supplier Material materials with Vicat softening temperature of 182 °C

ISO 306, VST B50

190 °C

Show Supplier Material materials with Vicat softening temperature of 190 °C

ISO 306, VST B50

Flammability

HB UL 94

Electrical

PropertyValueComment

Dielectric constant

3.5 [-]

Show Supplier Material materials with Dielectric constant of 3.5 [-]

DIN 53483

Dielectric strength

30 kV/mm

Show Supplier Material materials with Dielectric strength of 30 kV/mm

DIN53480

Loss tangent

0.038 [-]

Show Supplier Material materials with Loss tangent of 0.038 [-]

DIN 53483

Surface resistivity

1e+13 Ω/sq

Show Supplier Material materials with Surface resistivity of 1e+13 Ω/sq

DIN 53482

Volume resistivity

2.7e+14 Ω·cm

Show Supplier Material materials with Volume resistivity of 2.7e+14 Ω·cm

DIN 53482

Technological properties

Property
Certifications

RoHS,REACH