UHMWPE ISO-TECH

Alternative and trade names
ISO-LEN® 1000
Want to keep this datasheet? Save it now in your required format

Description

ISO-LEN® 1000 has been proven for many years in various fields of application. Due to its wide range of characteristics, this all-round material is being used in products in all areas of technology where particularly high demands on material are required. The key features are:


  • High abrasion resistance
  • Low friction coefficient
  • Self-lubricating
  • Very high notched impact strength
  • Related Standards

    This material data has been provided by ISO-TECH Kunststoff GmbH.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyTemperatureValueComment

    Coefficient of friction

    0.12 [-]

    Show Supplier Material materials with Coefficient of friction of 0.12 [-]

    DIN 53375, A, Against dry running steel

    Density

    23.0 °C

    0.93 g/cm³

    Show Supplier Material materials with Density of 0.93 g/cm³

    ISO 1183

    Water absorption

    23.0 °C

    0.01 %

    Show Supplier Material materials with Water absorption of 0.01 %

    ISO 62

    Mechanical

    PropertyTemperatureValueComment

    Elastic modulus

    23.0 °C

    0.7 GPa

    Show Supplier Material materials with Elastic modulus of 0.7 GPa

    min., ISO 527

    Elongation

    23.0 °C

    50 %

    Show Supplier Material materials with Elongation of 50 %

    min., ISO 527

    Elongation at yield

    23.0 °C

    8 %

    Show Supplier Material materials with Elongation at yield of 8 %

    min., ISO 527

    Flexural strength

    23.0 °C

    27 MPa

    Show Supplier Material materials with Flexural strength of 27 MPa

    ISO 178

    Hardness, Ball Indentation

    23.0 °C

    38 MPa

    Show Supplier Material materials with Hardness, Ball Indentation of 38 MPa

    ISO 2039-1

    Hardness, Shore D

    23.0 °C

    63 [-]

    Show Supplier Material materials with Hardness, Shore D of 63 [-]

    DIN 53505

    Tear strength

    23.0 °C

    40 kN/m

    Show Supplier Material materials with Tear strength of 40 kN/m

    min., ISO 527

    Yield strength

    23.0 °C

    17 MPa

    Show Supplier Material materials with Yield strength of 17 MPa

    ISO 527

    Impact strength, Charpy notched

    No break, ISO 179

    Impact strength, Charpy unnotched

    No break, ISO 179

    Thermal

    PropertyTemperatureValueComment

    Coefficient of thermal expansion

    23.0 °C

    2E-4 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 2E-4 1/K

    DIN 53752

    Heat deflection temperature, 0.45 MPa

    65 °C

    Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 65 °C

    Heat deflection temperature, 1.80 MPa

    42 °C

    Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 42 °C

    Max service temperature

    90 °C

    Show Supplier Material materials with Max service temperature of 90 °C

    Longterm

    Min service temperature

    -150 °C

    Show Supplier Material materials with Min service temperature of -150 °C

    Longterm

    Thermal conductivity

    23.0 °C

    0.41 W/(m·K)

    Show Supplier Material materials with Thermal conductivity of 0.41 W/(m·K)

    DIN 52612

    Vicat softening temperature

    79 °C

    Show Supplier Material materials with Vicat softening temperature of 79 °C

    ISO 306, VST B50

    Flammability

    HB UL 94

    Electrical

    PropertyTemperatureValueComment

    Dielectric constant, 1MHz

    23.0 °C

    3 [-]

    Show Supplier Material materials with Dielectric constant, 1MHz of 3 [-]

    DIN 53483

    Dielectric strength

    23.0 °C

    45 kV/mm

    Show Supplier Material materials with Dielectric strength of 45 kV/mm

    VDE 0303

    Loss tangent, 1MHz

    23.0 °C

    1E-4 [-]

    Show Supplier Material materials with Loss tangent, 1MHz of 1E-4 [-]

    DIN 53483

    Surface resistivity

    23.0 °C

    1.00E+11 Ω/sq

    Show Supplier Material materials with Surface resistivity of 1.00E+11 Ω/sq

    min., VDE 0303

    Volume resistivity

    23.0 °C

    1.00E+14 Ω·cm

    Show Supplier Material materials with Volume resistivity of 1.00E+14 Ω·cm

    min., VDE 0303

    Technological properties

    Property
    Application areas

    Sliding parts, chain guidance and sliding profiles

    Certifications

    Food Contact: FDA and EU 10/2011, RoHS,REACH