UHMWPE ISO-TECH M

Alternative and trade names
ISO-MOL®
Want to keep this datasheet? Save it now in your required format

Description

ISO-MOL® is a self-lubricating material based on a PE-UHMW with significantly improved sliding friction and abrasion resistance. Being an advancement of ISO-LEN® 1000, the addition of additives results in excellent wear behaviour and a very good sliding friction coefficient. ISO-MOL® is mainly used in plants where downtimes are very cost-intensive. In particular, slide rails and chain guide profiles as well as linings in the bulk goods sector are frequently produced on the basis of ISO-MOL®. The key features are:


  • Very low sliding friction coefficient
  • Higher abrasion resistance
  • Related Standards

    This material data has been provided by ISO-TECH Kunststoff GmbH.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyTemperatureValueComment

    Coefficient of friction

    0.08 [-]

    Show Supplier Material materials with Coefficient of friction of 0.08 [-]

    DIN 53375, A, Against dry running steel

    Density

    23.0 °C

    0.93 g/cm³

    Show Supplier Material materials with Density of 0.93 g/cm³

    ISO 1183

    Water absorption

    23.0 °C

    0.01 %

    Show Supplier Material materials with Water absorption of 0.01 %

    ISO 62

    Mechanical

    PropertyTemperatureValueComment

    Elastic modulus

    23.0 °C

    0.68 GPa

    Show Supplier Material materials with Elastic modulus of 0.68 GPa

    min., ISO 527

    Elongation at yield

    23.0 °C

    20 %

    Show Supplier Material materials with Elongation at yield of 20 %

    ISO 527

    Flexural strength

    23.0 °C

    27 MPa

    Show Supplier Material materials with Flexural strength of 27 MPa

    ISO 178

    Hardness, Ball Indentation

    23.0 °C

    35 MPa

    Show Supplier Material materials with Hardness, Ball Indentation of 35 MPa

    Hardness, Shore D

    23.0 °C

    61 [-]

    Show Supplier Material materials with Hardness, Shore D of 61 [-]

    DIN 53505

    Tensile strength

    23.0 °C

    28 MPa

    Show Supplier Material materials with Tensile strength of 28 MPa

    DIN 53455

    Yield strength

    23.0 °C

    17 MPa

    Show Supplier Material materials with Yield strength of 17 MPa

    ISO 527

    Elongation

    No break, ISO 527

    Impact strength, Charpy notched

    No break, ISO 179

    Impact strength, Charpy unnotched

    No break, ISO 179

    Tear strength

    No break, ISO 527

    Thermal

    PropertyTemperatureValueComment

    Coefficient of thermal expansion

    23.0 °C

    2E-4 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 2E-4 1/K

    DIN 53752

    Heat deflection temperature, 0.45 MPa

    42 °C

    Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 42 °C

    Max service temperature

    80 °C

    Show Supplier Material materials with Max service temperature of 80 °C

    Longterm

    Min service temperature

    -150 °C

    Show Supplier Material materials with Min service temperature of -150 °C

    Longterm

    Thermal conductivity

    23.0 °C

    0.41 W/(m·K)

    Show Supplier Material materials with Thermal conductivity of 0.41 W/(m·K)

    DIN 52612

    Vicat softening temperature

    80 °C

    Show Supplier Material materials with Vicat softening temperature of 80 °C

    ISO 306, VST B50

    Flammability

    HB UL 94

    Technological properties

    Property
    Application areas

    Sliding parts, chain guidance and sliding profiles

    Certifications

    Food Contact: FDA and EU 10/2011, RoHS,REACH