PA4.6 ISO-TECH

Alternative and trade names
ISO-MID PAPA4.6
Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by ISO-TECH Kunststoff GmbH.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueComment

Coefficient of friction

0.34 [-]

Show Supplier Material materials with Coefficient of friction of 0.34 [-]

DIN 53375, C, Against dry running steel

Density

1.18 g/cm³

Show Supplier Material materials with Density of 1.18 g/cm³

ISO 1183

Water absorption

3.7 %

Show Supplier Material materials with Water absorption of 3.7 %

ISO 62

Mechanical

PropertyValueComment

Elastic modulus

3 GPa

Show Supplier Material materials with Elastic modulus of 3 GPa

ISO 527

Hardness, Shore D

84 [-]

Show Supplier Material materials with Hardness, Shore D of 84 [-]

ISO 868

Impact strength, Charpy unnotched

6 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 6 kJ/m²

ISO 179

Yield strength

95 MPa

Show Supplier Material materials with Yield strength of 95 MPa

ISO 527

Thermal

PropertyValueComment

Max service temperature

155 °C

Show Supplier Material materials with Max service temperature of 155 °C

Longterm

Long

Short

Min service temperature

-40 °C

Show Supplier Material materials with Min service temperature of -40 °C

Longterm

Thermal conductivity

0.3 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 0.3 W/(m·K)

DIN 52612

Flammability

HB UL 94

Electrical

PropertyValueComment

Surface resistivity

1e+16 Ω/sq

Show Supplier Material materials with Surface resistivity of 1e+16 Ω/sq

DIN 60093

Technological properties

Property
Application areas

Sliding parts, rollers and bushings

Certifications