Description

Polybutylene Terephthalate (PBT) and Polyethylene Terephthalate (PET) alloy with 30% Glass Fiber Reinforced. Contains 25% Ocean Bound Plastic (OBP) PET Modification: Flame Retardant Grade

This material data has been provided by Lavergne.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.54 - 1.6 g/cm³

Show Supplier Material materials with Density of 1.54 - 1.6 g/cm³

ISO 1183

Recycled Content

25 %

Show Supplier Material materials with Recycled Content of 25 %

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

1.4 %

Show Supplier Material materials with Elongation of 1.4 %

ISO 527, 5 mm/min

Flexural modulus

23.0 °C

8.5 GPa

Show Supplier Material materials with Flexural modulus of 8.5 GPa

ISO 178, 2 mm/min

Flexural strength

23.0 °C

140 MPa

Show Supplier Material materials with Flexural strength of 140 MPa

ISO 178, 2 mm/min

Impact strength, Charpy notched

23.0 °C

6.4 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 6.4 kJ/m²

ISO 179eA

Impact strength, Izod notched

23.0 °C

5.9 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 5.9 kJ/m²

min., ISO 180

Tensile strength

23.0 °C

95 MPa

Show Supplier Material materials with Tensile strength of 95 MPa

ISO 527-2/1A, 10 mm/min

Thermal

PropertyTemperatureValueComment

Ash content

23.0 °C

30 - 35 %

Show Supplier Material materials with Ash content of 30 - 35 %

ASTM D5630

Heat deflection temperature, 0.45 MPa

205 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 205 °C

ISO 75

Melting point

242 °C

Show Supplier Material materials with Melting point of 242 °C

ISO 3146

Flammability

V-0 for 3.2 mm sample UL94

Electrical

PropertyTemperatureValueComment

Dielectric strength

23.0 °C

32 kV/mm

Show Supplier Material materials with Dielectric strength of 32 kV/mm

ASTM D149, 1.6 mm, 500V/s in oil

Dissipation factor, 1kHz

23.0 °C

2E-3 [-]

Show Supplier Material materials with Dissipation factor, 1kHz of 2E-3 [-]

ASTM D150

Volume resistivity

23.0 °C

1.00E+14 Ω·cm

Show Supplier Material materials with Volume resistivity of 1.00E+14 Ω·cm

ASTM D257

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.2 - 0.5 %

Show Supplier Material materials with Shrinkage of 0.2 - 0.5 %

ASTM D955

Shrinkage, transverse

23.0 °C

0.6 - 0.9 %

Show Supplier Material materials with Shrinkage, transverse of 0.6 - 0.9 %

ASTM D955

Technological properties

Property
Application areas

Electrical components (e.g. connectros) and structural components.

Certifications

RoHS,RECH,ULE Environmental Claims Validation

Color

Black

Fillers

30% Glass Fiber and Mineral Powder

Processing methods

  • Drying to Dew Point:-18°C or lower
  • Feed zone: 220-250°C
  • Middle zone: 230-260°C
  • Front zone: 240-265°C
  • Nozzle: 250-275°C
  • Melt temperature: 240-275°C
  • Mold temperature (thick wall parts): 40-120°C
  • Mold temperature (thin wall parts): ≥ 80°C cosmetic parts