VYPET™ VNT-615 HP

Alternative and trade names
PET-(GF+MD)15
Want to keep this datasheet? Save it now in your required format

Description

Polyethylene Terephthalate (PET) with 15% Glass Fiber Reinforced. Contains a minimum of 71% Post-consumer resin

This material data has been provided by Lavergne.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.4 g/cm³

Show Supplier Material materials with Density of 1.4 g/cm³

ISO 1183

Recycled Content

71 %

Show Supplier Material materials with Recycled Content of 71 %

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

6 GPa

Show Supplier Material materials with Flexural modulus of 6 GPa

ISO 178, 2 mm/min

Flexural strength

23.0 °C

150 MPa

Show Supplier Material materials with Flexural strength of 150 MPa

ISO 178, 2 mm/min

Impact strength, Izod notched

23.0 °C

6 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 6 kJ/m²

ISO 180

Tensile strength

23.0 °C

100 MPa

Show Supplier Material materials with Tensile strength of 100 MPa

ISO 527, 5 mm/min

Thermal

PropertyTemperatureValueComment

Ash content

23.0 °C

15 %

Show Supplier Material materials with Ash content of 15 %

ASTM D5630

Heat deflection temperature, 1.80 MPa

210 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 210 °C

ISO 75

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.4 %

Show Supplier Material materials with Shrinkage of 0.4 %

ASTM D955

Shrinkage, transverse

23.0 °C

0.8 %

Show Supplier Material materials with Shrinkage, transverse of 0.8 %

ASTM D955

Technological properties

Property
Application areas

Automotive structural parts (e.g. sunroof frames).

Certifications

RoHS,RECH

Color

Black

Fillers

15% Glass Fiber and Mineral Powder

Processing methods

  • Drying to Dew Point:-18°C or lower
  • Feed zone: 260-270°C
  • Middle zone: 265-275°C
  • Front zone: 270-290°C
  • Nozzle: 275-295°C
  • Melt temperature: 270-290°C Mold temperature (thick wall parts): 95-120°C
  • Mold temperature (thin wall parts): 95-120°C
  • Injection Pressure: Medium
  • Injection Speed: Medium
  • Back Pressure: Low
  • Speed: Medium