Polyethylene Terephthalate (PET) with 30% Glass Fiber Reinforced and Flame Retardant. Contains a minimum of 43% Post-consumer resin

This material data has been provided by Lavergne.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.68 g/cm³

Show Supplier Material materials with Density of 1.68 g/cm³

ISO 1183

Recycled Content

43 %

Show Supplier Material materials with Recycled Content of 43 %

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

10 GPa

Show Supplier Material materials with Flexural modulus of 10 GPa

ISO 178, 2 mm/min

Flexural strength

23.0 °C

190 MPa

Show Supplier Material materials with Flexural strength of 190 MPa

ISO 178, 2 mm/min

Impact strength, Izod notched

23.0 °C

8.5 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 8.5 kJ/m²

ISO 180

Tensile strength

23.0 °C

125 MPa

Show Supplier Material materials with Tensile strength of 125 MPa

ISO 527, 5 mm/min

Thermal

PropertyTemperatureValueComment

Ash content

23.0 °C

30 %

Show Supplier Material materials with Ash content of 30 %

ASTM D5630

Heat deflection temperature, 1.80 MPa

220 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 220 °C

ISO 75

Flammability

V0, V0 5VA for 3.2 mm sample UL94

Electrical

PropertyTemperatureValueComment

Dielectric strength

23.0 °C

29 kV/mm

Show Supplier Material materials with Dielectric strength of 29 kV/mm

ASTM D149, 1.6 mm, 500V/s in oil

Volume resistivity

23.0 °C

1.00E+16 Ω·cm

Show Supplier Material materials with Volume resistivity of 1.00E+16 Ω·cm

ASTM D257

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.3 %

Show Supplier Material materials with Shrinkage of 0.3 %

ASTM D955

Shrinkage, transverse

23.0 °C

0.8 %

Show Supplier Material materials with Shrinkage, transverse of 0.8 %

ASTM D955

Technological properties

Property
Application areas

Electrical components, appliances and structral applications.

Certifications

RoHS,RECH,ULE Environmental Claims Validation

Color

Black

Fillers

30% Glass Fiber

Processing methods

  • Drying to Dew Point:-18°C or lower
  • Feed zone: 260-270°C
  • Middle zone: 265-275°C
  • Front zone: 270-290°C
  • Nozzle: 275-295°C
  • Melt temperature: 275-295°C
  • Mold temperature (thick wall parts): 95-120°C
  • Mold temperature (thin wall parts): 95-120°C
  • Injection Pressure: 55-85 MPa
  • Injection Speed: Fast
  • Back Pressure: 25-50 psi
  • Screw Speed: 50-75 rpm