General
Property | Temperature | Value | Related Standards |
---|---|---|---|
Density | 20.0 °C | 2.73 g/cm³ Show Material materials with Density of 2.73 g/cm³ | EN 573-3 |
Mechanical
Property | Temperature | Value | Related Standards | Comment |
---|---|---|---|---|
Elastic modulus | -270.0 °C | 70.0 GPa Show Material materials with Elastic modulus of 70.0 GPa | EN 573-3 | |
20.0 °C | 60.0 - 70.0 GPa Show Material materials with Elastic modulus of 60.0 - 70.0 GPa | EN 573-3 | ||
20.0 °C | 60.0 - 65.0 GPa Show Material materials with Elastic modulus of 60.0 - 65.0 GPa | EN 573-3 | ||
20.0 °C | 60.0 - 69.5 GPa Show Material materials with Elastic modulus of 60.0 - 69.5 GPa | EN 573-3 | ||
20.0 °C | 60.0 - 69.0 GPa Show Material materials with Elastic modulus of 60.0 - 69.0 GPa | EN 573-3 | ||
20.0 °C | 65.0 - 70.0 GPa Show Material materials with Elastic modulus of 65.0 - 70.0 GPa | EN 573-3 | ||
20.0 °C | 65.0 - 69.5 GPa Show Material materials with Elastic modulus of 65.0 - 69.5 GPa | EN 573-3 | ||
20.0 °C | 65.0 - 69.0 GPa Show Material materials with Elastic modulus of 65.0 - 69.0 GPa | EN 573-3 | ||
20.0 °C | 69.0 GPa Show Material materials with Elastic modulus of 69.0 GPa | EN 573-3 | ||
20.0 °C | 69.0 - 70.0 GPa Show Material materials with Elastic modulus of 69.0 - 70.0 GPa | EN 573-3 | ||
20.0 °C | 69.0 - 69.5 GPa Show Material materials with Elastic modulus of 69.0 - 69.5 GPa | EN 573-3 | ||
20.0 °C | 69.5 - 70.0 GPa Show Material materials with Elastic modulus of 69.5 - 70.0 GPa | EN 573-3 | ||
20.0 °C | 69.5 GPa Show Material materials with Elastic modulus of 69.5 GPa | EN 573-3 | ||
20.0 °C | 70.0 GPa Show Material materials with Elastic modulus of 70.0 GPa | EN 573-3 | ||
50.0 °C | 69.0 GPa Show Material materials with Elastic modulus of 69.0 GPa | EN 573-3 | ||
100.0 °C | 68.0 GPa Show Material materials with Elastic modulus of 68.0 GPa | EN 573-3 | ||
150.0 °C | 66.0 GPa Show Material materials with Elastic modulus of 66.0 GPa | EN 573-3 | ||
200.0 °C | 63.0 GPa Show Material materials with Elastic modulus of 63.0 GPa | EN 573-3 | ||
250.0 °C | 57.0 GPa Show Material materials with Elastic modulus of 57.0 GPa | EN 573-3 | ||
300.0 °C | 50.0 GPa Show Material materials with Elastic modulus of 50.0 GPa | EN 573-3 | ||
Elongation | -196.0 °C | 23.0 - 30.0 % Show Material materials with Elongation of 23.0 - 30.0 % | EN 573-3 | |
-196.0 °C | 23.0 % Show Material materials with Elongation of 23.0 % | EN 573-3 | ||
-196.0 °C | 30.0 % Show Material materials with Elongation of 30.0 % | EN 573-3 | ||
-80.0 °C | 11.0 - 18.0 % Show Material materials with Elongation of 11.0 - 18.0 % | EN 573-3 | ||
-80.0 °C | 11.0 % Show Material materials with Elongation of 11.0 % | EN 573-3 | ||
-80.0 °C | 18.0 % Show Material materials with Elongation of 18.0 % | EN 573-3 | ||
-28.0 °C | 10.0 - 16.0 % Show Material materials with Elongation of 10.0 - 16.0 % | EN 573-3 | ||
-28.0 °C | 10.0 % Show Material materials with Elongation of 10.0 % | EN 573-3 | ||
-28.0 °C | 16.0 % Show Material materials with Elongation of 16.0 % | EN 573-3 | ||
20.0 °C | 10.0 - 16.0 % Show Material materials with Elongation of 10.0 - 16.0 % | EN 573-3 | ||
20.0 °C | 10.0 % Show Material materials with Elongation of 10.0 % | EN 573-3 | ||
20.0 °C | 16.0 % Show Material materials with Elongation of 16.0 % | EN 573-3 | ||
100.0 °C | 10.0 - 16.0 % Show Material materials with Elongation of 10.0 - 16.0 % | EN 573-3 | ||
100.0 °C | 10.0 % Show Material materials with Elongation of 10.0 % | EN 573-3 | ||
100.0 °C | 16.0 % Show Material materials with Elongation of 16.0 % | EN 573-3 | ||
150.0 °C | 11.0 % Show Material materials with Elongation of 11.0 % | EN 573-3 | ||
150.0 °C | 11.0 - 16.0 % Show Material materials with Elongation of 11.0 - 16.0 % | EN 573-3 | ||
150.0 °C | 16.0 % Show Material materials with Elongation of 16.0 % | EN 573-3 | ||
200.0 °C | 18.0 % Show Material materials with Elongation of 18.0 % | EN 573-3 | ||
200.0 °C | 18.0 - 20.0 % Show Material materials with Elongation of 18.0 - 20.0 % | EN 573-3 | ||
200.0 °C | 20.0 % Show Material materials with Elongation of 20.0 % | EN 573-3 | ||
260.0 °C | 60.0 % Show Material materials with Elongation of 60.0 % | EN 573-3 | ||
315.0 °C | 70.0 % Show Material materials with Elongation of 70.0 % | EN 573-3 | ||
370.0 °C | 70.0 % Show Material materials with Elongation of 70.0 % | EN 573-3 | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 3000 Series Aluminium | ||
Poisson's ratio | 20.0 °C | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | EN 573-3 | |
Shear modulus | 20.0 °C | 24.0 - 26.5 GPa Show Material materials with Shear modulus of 24.0 - 26.5 GPa | EN 573-3 | |
20.0 °C | 24.0 - 26.1 GPa Show Material materials with Shear modulus of 24.0 - 26.1 GPa | EN 573-3 | ||
20.0 °C | 26.1 - 26.5 GPa Show Material materials with Shear modulus of 26.1 - 26.5 GPa | EN 573-3 | ||
20.0 °C | 26.1 GPa Show Material materials with Shear modulus of 26.1 GPa | EN 573-3 | ||
Tensile strength | -196.0 °C | 240.0 MPa Show Material materials with Tensile strength of 240.0 MPa | EN 573-3 | |
-196.0 °C | 240.0 - 280.0 MPa Show Material materials with Tensile strength of 240.0 - 280.0 MPa | EN 573-3 | ||
-196.0 °C | 280.0 MPa Show Material materials with Tensile strength of 280.0 MPa | EN 573-3 | ||
-80.0 °C | 165.0 MPa Show Material materials with Tensile strength of 165.0 MPa | EN 573-3 | ||
-80.0 °C | 165.0 - 220.0 MPa Show Material materials with Tensile strength of 165.0 - 220.0 MPa | EN 573-3 | ||
-80.0 °C | 220.0 MPa Show Material materials with Tensile strength of 220.0 MPa | EN 573-3 | ||
-28.0 °C | 150.0 MPa Show Material materials with Tensile strength of 150.0 MPa | EN 573-3 | ||
-28.0 °C | 150.0 - 205.0 MPa Show Material materials with Tensile strength of 150.0 - 205.0 MPa | EN 573-3 | ||
-28.0 °C | 205.0 MPa Show Material materials with Tensile strength of 205.0 MPa | EN 573-3 | ||
128.0 MPa Show Material materials with Tensile strength of 128.0 MPa | ||||
20.0 °C | 150.0 MPa Show Material materials with Tensile strength of 150.0 MPa | EN 573-3 | ||
20.0 °C | 150.0 - 200.0 MPa Show Material materials with Tensile strength of 150.0 - 200.0 MPa | EN 573-3 | ||
20.0 °C | 200.0 MPa Show Material materials with Tensile strength of 200.0 MPa | EN 573-3 | ||
100.0 °C | 145.0 MPa Show Material materials with Tensile strength of 145.0 MPa | EN 573-3 | ||
100.0 °C | 145.0 - 180.0 MPa Show Material materials with Tensile strength of 145.0 - 180.0 MPa | EN 573-3 | ||
100.0 °C | 180.0 MPa Show Material materials with Tensile strength of 180.0 MPa | EN 573-3 | ||
150.0 °C | 125.0 MPa Show Material materials with Tensile strength of 125.0 MPa | EN 573-3 | ||
150.0 °C | 125.0 - 160.0 MPa Show Material materials with Tensile strength of 125.0 - 160.0 MPa | EN 573-3 | ||
150.0 °C | 160.0 MPa Show Material materials with Tensile strength of 160.0 MPa | EN 573-3 | ||
200.0 °C | 95.0 MPa Show Material materials with Tensile strength of 95.0 MPa | EN 573-3 | ||
260.0 °C | 50.0 MPa Show Material materials with Tensile strength of 50.0 MPa | EN 573-3 | ||
315.0 °C | 30.0 MPa Show Material materials with Tensile strength of 30.0 MPa | EN 573-3 | ||
370.0 °C | 20.0 MPa Show Material materials with Tensile strength of 20.0 MPa | EN 573-3 | ||
Yield strength | -196.0 °C | 170.0 MPa Show Material materials with Yield strength of 170.0 MPa | EN 573-3 | RP02 |
-196.0 °C | 170.0 - 230.0 MPa Show Material materials with Yield strength of 170.0 - 230.0 MPa | EN 573-3 | RP02 | |
-196.0 °C | 230.0 MPa Show Material materials with Yield strength of 230.0 MPa | EN 573-3 | RP02 | |
-80.0 °C | 150.0 MPa Show Material materials with Yield strength of 150.0 MPa | EN 573-3 | RP02 | |
-80.0 °C | 150.0 - 200.0 MPa Show Material materials with Yield strength of 150.0 - 200.0 MPa | EN 573-3 | RP02 | |
-80.0 °C | 200.0 MPa Show Material materials with Yield strength of 200.0 MPa | EN 573-3 | RP02 | |
-28.0 °C | 140.0 MPa Show Material materials with Yield strength of 140.0 MPa | EN 573-3 | RP02 | |
-28.0 °C | 140.0 - 190.0 MPa Show Material materials with Yield strength of 140.0 - 190.0 MPa | EN 573-3 | RP02 | |
-28.0 °C | 190.0 MPa Show Material materials with Yield strength of 190.0 MPa | EN 573-3 | RP02 | |
57.0 MPa Show Material materials with Yield strength of 57.0 MPa | ||||
20.0 °C | 140.0 MPa Show Material materials with Yield strength of 140.0 MPa | EN 573-3 | RP02 | |
20.0 °C | 140.0 - 185.0 MPa Show Material materials with Yield strength of 140.0 - 185.0 MPa | EN 573-3 | RP02 | |
20.0 °C | 185.0 MPa Show Material materials with Yield strength of 185.0 MPa | EN 573-3 | RP02 | |
100.0 °C | 130.0 MPa Show Material materials with Yield strength of 130.0 MPa | EN 573-3 | RP02 | |
100.0 °C | 130.0 - 145.0 MPa Show Material materials with Yield strength of 130.0 - 145.0 MPa | EN 573-3 | RP02 | |
100.0 °C | 145.0 MPa Show Material materials with Yield strength of 145.0 MPa | EN 573-3 | RP02 | |
150.0 °C | 110.0 MPa Show Material materials with Yield strength of 110.0 MPa | EN 573-3 | RP02 | |
200.0 °C | 60.0 MPa Show Material materials with Yield strength of 60.0 MPa | EN 573-3 | RP02 | |
260.0 °C | 30.0 MPa Show Material materials with Yield strength of 30.0 MPa | EN 573-3 | RP02 | |
315.0 °C | 15.0 MPa Show Material materials with Yield strength of 15.0 MPa | EN 573-3 | RP02 | |
370.0 °C | 10.0 MPa Show Material materials with Yield strength of 10.0 MPa | EN 573-3 | RP02 |
Thermal
Property | Temperature | Value | Related Standards | Comment |
---|---|---|---|---|
Coefficient of thermal expansion | -50.0 °C | 2.15e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.15e-05 1/K | EN 573-3 | |
2.33e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.33e-05 1/K | ||||
100.0 °C | 2.32e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.32e-05 1/K | EN 573-3 | ||
200.0 °C | 2.41e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.41e-05 1/K | EN 573-3 | ||
300.0 °C | 2.52e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.52e-05 1/K | EN 573-3 | ||
Melting point | 629.0 - 654.0 °C Show Material materials with Melting point of 629.0 - 654.0 °C | Typical for Wrought 3000 Series Aluminium | ||
Specific heat capacity | 20.0 °C | 892.0 - 893.0 J/(kg·K) Show Material materials with Specific heat capacity of 892.0 - 893.0 J/(kg·K) | EN 573-3 | |
20.0 °C | 892.0 J/(kg·K) Show Material materials with Specific heat capacity of 892.0 J/(kg·K) | EN 573-3 | ||
20.0 °C | 893.0 J/(kg·K) Show Material materials with Specific heat capacity of 893.0 J/(kg·K) | EN 573-3 | ||
Thermal conductivity | 175.0 W/(m·K) Show Material materials with Thermal conductivity of 175.0 W/(m·K) | |||
20.0 °C | 160.0 - 200.0 W/(m·K) Show Material materials with Thermal conductivity of 160.0 - 200.0 W/(m·K) | EN 573-3 | ||
20.0 °C | 160.0 W/(m·K) Show Material materials with Thermal conductivity of 160.0 W/(m·K) | EN 573-3 |
Electrical
Property | Temperature | Value | Related Standards |
---|---|---|---|
Electrical conductivity | 20.0 °C | 22000000.0 - 29000000.0 S/m Show Material materials with Electrical conductivity of 22000000.0 - 29000000.0 S/m | EN 573-3 |
20.0 °C | 23000000.0 - 29000000.0 S/m Show Material materials with Electrical conductivity of 23000000.0 - 29000000.0 S/m | EN 573-3 | |
Electrical resistivity | 20.0 °C | 3.4e-08 - 4.1e-08 Ω·m Show Material materials with Electrical resistivity of 3.4e-08 - 4.1e-08 Ω·m | EN 573-3 |
20.0 °C | 3.4e-08 - 4.5e-08 Ω·m Show Material materials with Electrical resistivity of 3.4e-08 - 4.5e-08 Ω·m | EN 573-3 | |
20.0 °C | 4.1e-08 Ω·m Show Material materials with Electrical resistivity of 4.1e-08 Ω·m | EN 573-3 | |
20.0 °C | 4.1e-08 - 4.5e-08 Ω·m Show Material materials with Electrical resistivity of 4.1e-08 - 4.5e-08 Ω·m | EN 573-3 |
Chemical properties
Property | Value | Related Standards |
---|---|---|
Copper | 0.05 - 0.2 % Show Material materials with Copper of 0.05 - 0.2 % | EN 573-3 |
Iron | 0.7 Show Material materials with Iron of 0.7 | EN 573-3 |
Manganese | 1.0 - 1.5 % Show Material materials with Manganese of 1.0 - 1.5 % | EN 573-3 |
Silicon | 0.6 Show Material materials with Silicon of 0.6 | EN 573-3 |
Zinc | 0.1 Show Material materials with Zinc of 0.1 | EN 573-3 |
Technological properties
Property | ||
---|---|---|
Workability | Good workability. |