Naturally hard AlSi alloy. The alloy is food safe.

Related Standards

Equivalent Materials

This material data has been provided by WIAM,AluKey,Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueRelated StandardsShape

Density

2.68 g/cm³

Show Material materials with Density of 2.68 g/cm³

EN 573-3

Strip, Sheet, Plate

2.68 g/cm³

Show Material materials with Density of 2.68 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

69.0 GPa

Show Material materials with Elastic modulus of 69.0 GPa

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 4000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 4000 Series Aluminium

Shear modulus

26.0 GPa

Show Material materials with Shear modulus of 26.0 GPa

Typical for Wrought 4000 Series Aluminium

Tensile strength

110.0 MPa

Show Material materials with Tensile strength of 110.0 MPa

Yield strength

70.0 MPa

Show Material materials with Yield strength of 70.0 MPa

Thermal

PropertyTemperatureValueRelated StandardsShape

Coefficient of thermal expansion

2.1600000000000003e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.1600000000000003e-05 1/K

20 °C

2.16e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.16e-05 1/K

EN 573-3

Strip, Sheet, Plate

100 °C

2.16e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.16e-05 1/K

EN 573-3

Strip, Sheet, Plate

Melting point

575.0 - 615.0 °C

Show Material materials with Melting point of 575.0 - 615.0 °C

EN 573-3

Strip, Sheet, Plate

Specific heat capacity

890.0 J/(kg·K)

Show Material materials with Specific heat capacity of 890.0 J/(kg·K)

Thermal conductivity

180 W/(m·K)

Show Material materials with Thermal conductivity of 180 W/(m·K)

EN 573-3

Strip, Sheet, Plate

180.0 W/(m·K)

Show Material materials with Thermal conductivity of 180.0 W/(m·K)

Electrical

PropertyValueRelated StandardsShape

Electrical conductivity

27000000.0 S/m

Show Material materials with Electrical conductivity of 27000000.0 S/m

EN 573-3

Strip, Sheet, Plate

Electrical resistivity

3.7e-08 Ω·m

Show Material materials with Electrical resistivity of 3.7e-08 Ω·m

EN 573-3

Strip, Sheet, Plate

Chemical properties

PropertyValueRelated StandardsShape

Copper

0.25 %

Show Material materials with Copper of 0.25 %

EN 573-3

Strip, Sheet, Plate

Iron

0.8 %

Show Material materials with Iron of 0.8 %

EN 573-3

0.80 %

Show Material materials with Iron of 0.80 %

EN 573-3

Strip, Sheet, Plate

Manganese

0.1 %

Show Material materials with Manganese of 0.1 %

EN 573-3

Strip, Sheet, Plate

Silicon

6.8 - 8.2 %

Show Material materials with Silicon of 6.8 - 8.2 %

EN 573-3

Strip, Sheet, Plate

Zinc

0.2 %

Show Material materials with Zinc of 0.2 %

EN 573-3

Strip, Sheet, Plate

Technological properties

Property
Workability

Moderate Workability

Looking for suppliers of this material? Click to see 1 supplier of EN 573-3 Grade AW-4343 on Matmatch