DIN 5513 Grade AW-5754

View suppliers (45)
Want to keep this datasheet? Save it now in your required format

Description

Application note for rail vehicles (according to DIN 5513 for H111, H112, H12, H22 conditions): - for roof and side walls - observe the decrease in strength in heat affected zone in H112, H12 and H22 conditions - good chemical resistance, good cold formability in the H111, H112 and H22 conditions The material can be anodised.

Related Standards

Equivalent Materials

This material data has been provided by WIAM,Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

2.67 g/cm³

Show Material materials with Density of 2.67 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

70.0 GPa

Show Material materials with Elastic modulus of 70.0 GPa

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 5000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 5000 Series Aluminium

Shear modulus

26.0 - 26.5 GPa

Show Material materials with Shear modulus of 26.0 - 26.5 GPa

Typical for Wrought 5000 Series Aluminium

Tensile strength

115.0 MPa

Show Material materials with Tensile strength of 115.0 MPa

Yield strength

80.0 MPa

Show Material materials with Yield strength of 80.0 MPa

Thermal

PropertyValueComment

Coefficient of thermal expansion

2.3800000000000003e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.3800000000000003e-05 1/K

Max service temperature

150.0 °C

Show Material materials with Max service temperature of 150.0 °C

Typical for Wrought 5000 Series Aluminium

Melting point

560.0 - 655.0 °C

Show Material materials with Melting point of 560.0 - 655.0 °C

Typical for Wrought 5000 Series Aluminium

Specific heat capacity

900.0 J/(kg·K)

Show Material materials with Specific heat capacity of 900.0 J/(kg·K)

Thermal conductivity

145.0 W/(m·K)

Show Material materials with Thermal conductivity of 145.0 W/(m·K)

Electrical

PropertyValueComment

Electrical conductivity

18000000.0 - 31000000.0 S/m

Show Material materials with Electrical conductivity of 18000000.0 - 31000000.0 S/m

Typical for Wrought 5000 Series Aluminium

Electrical resistivity

3.3e-08 - 5e-08 Ω·m

Show Material materials with Electrical resistivity of 3.3e-08 - 5e-08 Ω·m

Typical for Wrought 5000 Series Aluminium

Technological properties

Property
Workability

Good workability.