General
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Density | 2.7 g/cm³ Show Material materials with Density of 2.7 g/cm³ | T6 | BS 1474 | Bar, Tube, Plate |
Mechanical
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Elastic modulus | 70 GPa Show Material materials with Elastic modulus of 70 GPa | T6 | BS 1474 | Bar, Tube, Plate | |
Elongation | 6.0 - 8.0 % Show Material materials with Elongation of 6.0 - 8.0 % | T6 | BS 1474 | Bar, Tube, Plate | |
Hardness, Brinell | 84.0 - 91.0 [-] Show Material materials with Hardness, Brinell of 84.0 - 91.0 [-] | T6 | BS 1474 | Bar, Tube, Plate | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 6000 Series Aluminium | |||
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Wrought 6000 Series Aluminium | |||
Shear modulus | 26.0 - 26.5 GPa Show Material materials with Shear modulus of 26.0 - 26.5 GPa | Typical for Wrought 6000 Series Aluminium | |||
Tensile strength | 310 MPa Show Material materials with Tensile strength of 310 MPa | T6 | BS 1474 | Bar, Tube, Plate | |
Yield strength | 270 MPa Show Material materials with Yield strength of 270 MPa | T6 | BS 1474 | Bar, Tube, Plate |
Thermal
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | 2.4e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.4e-05 1/K | T6 | BS 1474 | Bar, Tube, Plate | |
Melting point | 555.0 °C Show Material materials with Melting point of 555.0 °C | T6 | BS 1474 | Bar, Tube, Plate | |
Specific heat capacity | 887.0 - 963.0 J/(kg·K) Show Material materials with Specific heat capacity of 887.0 - 963.0 J/(kg·K) | Typical for Wrought 6000 Series Aluminium | |||
Thermal conductivity | 180 W/(m·K) Show Material materials with Thermal conductivity of 180 W/(m·K) | T6 | BS 1474 | Bar, Tube, Plate |
Electrical
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Electrical conductivity | 21000000.0 - 34000000.0 S/m Show Material materials with Electrical conductivity of 21000000.0 - 34000000.0 S/m | Typical for Wrought 6000 Series Aluminium | |||
Electrical resistivity | 3.7999999999999996e-08 Ω·m Show Material materials with Electrical resistivity of 3.7999999999999996e-08 Ω·m | T6 | BS 1474 | Bar, Tube, Plate |
Chemical properties
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Chromium | 0.25 Show Material materials with Chromium of 0.25 | T6 | BS 1474 | Bar, Tube, Plate | |
Copper | 0.1 Show Material materials with Copper of 0.1 | T6 | BS 1474 | Bar, Tube, Plate | |
Iron | 0.5 Show Material materials with Iron of 0.5 | T6 | BS 1474 | Bar, Tube, Plate | |
Magnesium | 0.6 - 1.2 % Show Material materials with Magnesium of 0.6 - 1.2 % | T6 | BS 1474 | Bar, Tube, Plate | |
Manganese | 0.4 - 1.0 % Show Material materials with Manganese of 0.4 - 1.0 % | T6 | BS 1474 | Bar, Tube, Plate | |
Other | 0.15 Show Material materials with Other of 0.15 | T6 | BS 1474 | Bar, Tube, Plate | Total |
Silicon | 0.7 - 1.3 % Show Material materials with Silicon of 0.7 - 1.3 % | T6 | BS 1474 | Bar, Tube, Plate | |
Titanium | 0.1 Show Material materials with Titanium of 0.1 | T6 | BS 1474 | Bar, Tube, Plate | |
Zinc | 0.2 Show Material materials with Zinc of 0.2 | T6 | BS 1474 | Bar, Tube, Plate |
Technological properties
Property | ||
---|---|---|
Workability | Excellent workability. |