General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Density | 2.71 g/cm³ Show Material materials with Density of 2.71 g/cm³ | H44 | EN 573-3, EN 1396, EN 541 | Strip, Sheet, Plate, Foil | |
20.0 °C | 2.71 g/cm³ Show Material materials with Density of 2.71 g/cm³ | H44 | EN 573-3 | Sheet, Strip |
Mechanical
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Elastic modulus | 70.0 GPa Show Material materials with Elastic modulus of 70.0 GPa | H44 | EN 573-3, EN 1396, EN 541 | Strip, Sheet, Plate, Foil | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 8000 Series Aluminium | ||||
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Wrought 8000 Series Aluminium | ||||
Tensile strength | 110.0 - 150.0 MPa Show Material materials with Tensile strength of 110.0 - 150.0 MPa | H44 | EN 573-3, EN 541 | Strip, Sheet, Plate, Foil | ||
20.0 °C | 120.0 - 160.0 MPa Show Material materials with Tensile strength of 120.0 - 160.0 MPa | H44 | EN 573-3, EN 541 | Sheet, Strip, Plate, Foil | ||
20.0 °C | 125.0 - 165.0 MPa Show Material materials with Tensile strength of 125.0 - 165.0 MPa | H44 | EN 573-3 | Sheet, Strip | Transverse | |
20.0 °C | 125.0 - 165.0 MPa Show Material materials with Tensile strength of 125.0 - 165.0 MPa | H44 | EN 573-3, EN 1396 | Sheet, Strip, Plate, Foil |
Thermal
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coefficient of thermal expansion | 20 °C | 2.35e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.35e-05 1/K | H44 | EN 573-3, EN 1396, EN 541 | Strip, Sheet, Plate, Foil | |
100 °C | 2.35e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.35e-05 1/K | H44 | EN 573-3, EN 1396, EN 541 | Strip, Sheet, Plate, Foil | ||
Melting point | 640.0 - 655.0 °C Show Material materials with Melting point of 640.0 - 655.0 °C | H44 | EN 573-3, EN 1396, EN 541 | Strip, Sheet, Plate, Foil | ||
Specific heat capacity | 920.0 J/(kg·K) Show Material materials with Specific heat capacity of 920.0 J/(kg·K) | Typical for Wrought 8000 Series Aluminium | ||||
Thermal conductivity | 20.0 °C | 210.0 - 220.0 W/(m·K) Show Material materials with Thermal conductivity of 210.0 - 220.0 W/(m·K) | H44 | EN 573-3, EN 1396, EN 541 | Sheet, Strip, Plate, Foil |
Electrical
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Electrical conductivity | 20.0 °C | 34000000.0 - 35000000.0 S/m Show Material materials with Electrical conductivity of 34000000.0 - 35000000.0 S/m | H44 | EN 573-3, EN 1396, EN 541 | Sheet, Strip, Plate, Foil |
Electrical resistivity | 2.86e-08 - 2.94e-08 Ω·m Show Material materials with Electrical resistivity of 2.86e-08 - 2.94e-08 Ω·m | H44 | EN 573-3, EN 1396, EN 541 | Strip, Sheet, Plate, Foil |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chromium | 0.1 % Show Material materials with Chromium of 0.1 % | H44 | EN 573-3, EN 1396, EN 541 | Sheet, Strip, Plate, Foil |
Copper | 0.1 % Show Material materials with Copper of 0.1 % | H44 | EN 573-3, EN 1396, EN 541 | Sheet, Strip, Plate, Foil |
Iron | 0.5 - 1.0 % Show Material materials with Iron of 0.5 - 1.0 % | H44 | EN 573-3, EN 1396, EN 541 | Sheet, Strip, Plate, Foil |
Magnesium | 0.1 % Show Material materials with Magnesium of 0.1 % | H44 | EN 573-3, EN 1396, EN 541 | Sheet, Strip, Plate, Foil |
Manganese | 0.1 % Show Material materials with Manganese of 0.1 % | H44 | EN 573-3, EN 1396, EN 541 | Sheet, Strip, Plate, Foil |
Silicon | 0.4 - 0.8 % Show Material materials with Silicon of 0.4 - 0.8 % | H44 | EN 573-3, EN 1396, EN 541 | Sheet, Strip, Plate, Foil |
Titanium | 0.05 % Show Material materials with Titanium of 0.05 % | H44 | EN 573-3, EN 1396, EN 541 | Sheet, Strip, Plate, Foil |
Zinc | 0.1 % Show Material materials with Zinc of 0.1 % | H44 | EN 573-3, EN 1396, EN 541 | Sheet, Strip, Plate, Foil |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: acceptable, Protective: very good | |
Brazing | hard brazing (with flux/ without flux): very good / very good, friction soldering: very good, soft brazing with flux: very good | |
Corrosion properties | Seawater: sufficient, weathering: acceptable | |
Workability | Bending / Spinning (cold): good / good, Impact extrusion (cold): good, Deep drawing / upsetting (Condition) good (H14) / good (H14) |