Description

Alloyed aluminium ingots for remelting.

Related Standards

Equivalent Materials

This material data has been provided by WIAM,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueComment

Density

2.6 - 2.7 g/cm³

Show Material materials with Density of 2.6 - 2.7 g/cm³

Typical for Cast 5xx.x Series Aluminium

Mechanical

PropertyValueComment

Elastic modulus

68.0 - 70.0 GPa

Show Material materials with Elastic modulus of 68.0 - 70.0 GPa

Typical for Cast 5xx.x Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Cast 5xx.x Series Aluminium

Thermal

PropertyValueComment

Coefficient of thermal expansion

2.3e-05 - 2.5e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.3e-05 - 2.5e-05 1/K

Typical for Cast 5xx.x Series Aluminium

Melting point

450.0 - 640.0 °C

Show Material materials with Melting point of 450.0 - 640.0 °C

Typical for Cast 5xx.x Series Aluminium

Specific heat capacity

963.0 J/(kg·K)

Show Material materials with Specific heat capacity of 963.0 J/(kg·K)

Typical for Cast 5xx.x Series Aluminium

Thermal conductivity

60.0 - 140.0 W/(m·K)

Show Material materials with Thermal conductivity of 60.0 - 140.0 W/(m·K)

Typical for Cast 5xx.x Series Aluminium

Chemical properties

PropertyValueRelated Standards

Copper

0.03 %

Show Material materials with Copper of 0.03 %

EN 1676

0.08 %

Show Material materials with Copper of 0.08 %

EN 1676

Iron

0.4 %

Show Material materials with Iron of 0.4 %

EN 1676

0.45 - 0.9 %

Show Material materials with Iron of 0.45 - 0.9 %

EN 1676

Lead

0.1 %

Show Material materials with Lead of 0.1 %

EN 1676

Magnesium

2.7 - 3.5 %

Show Material materials with Magnesium of 2.7 - 3.5 %

EN 1676

8.5 - 10.5 %

Show Material materials with Magnesium of 8.5 - 10.5 %

EN 1676

Manganese

0.45 %

Show Material materials with Manganese of 0.45 %

EN 1676

0.55 %

Show Material materials with Manganese of 0.55 %

EN 1676

Nickel

0.1 %

Show Material materials with Nickel of 0.1 %

EN 1676

Silicon

0.45 %

Show Material materials with Silicon of 0.45 %

EN 1676

2.5 %

Show Material materials with Silicon of 2.5 %

EN 1676

Tin

0.1 %

Show Material materials with Tin of 0.1 %

EN 1676

Titanium

0.15 %

Show Material materials with Titanium of 0.15 %

EN 1676

Zinc

0.1 %

Show Material materials with Zinc of 0.1 %

EN 1676

0.25 %

Show Material materials with Zinc of 0.25 %