ASTM B210 Grade 5154 H34

.XLSX
.PDF
Save

Description

Related Standards

Properties

Mechanical

Elongation A50 A50

0 - 5 % at 20 °C

Tensile strength Rm

0 - 270 MPa at 20 °C

Yield Strength Rp0.2, short transverse Rp0.2,shorttrans_

0 - 200 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Mg

3.1 - 3.9 %

Cr

0.15 - 0.35 %

Cu

0 - 0.1 %

Fe

0 - 0.4 %

Mn

0 - 0.1 %

More

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.