General
Property | Value | Comment |
---|---|---|
Density | 2.7 g/cm³ Show Material materials with Density of 2.7 g/cm³ | Typical for Wrought 1000 Series Aluminium |
Mechanical
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Elastic modulus | 68.0 - 70.0 GPa Show Material materials with Elastic modulus of 68.0 - 70.0 GPa | Typical for Wrought 1000 Series Aluminium | |||
Elongation | 22.0 % Show Material materials with Elongation of 22.0 % | O | ASTM B211 | Bar, Rod, Wire | |
25.0 % Show Material materials with Elongation of 25.0 % | O | ASTM B211 | Bar, Rod, Wire | A50 | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 1000 Series Aluminium | |||
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Wrought 1000 Series Aluminium | |||
Shear modulus | 25.9 GPa Show Material materials with Shear modulus of 25.9 GPa | Typical for Wrought 1000 Series Aluminium | |||
Tensile strength | 75.0 - 105.0 MPa Show Material materials with Tensile strength of 75.0 - 105.0 MPa | O | ASTM B211 | Bar, Rod, Wire |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 2.2e-05 - 2.5e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.2e-05 - 2.5e-05 1/K | Typical for Wrought 1000 Series Aluminium |
Melting point | 645.0 - 660.0 °C Show Material materials with Melting point of 645.0 - 660.0 °C | Typical for Wrought 1000 Series Aluminium |
Specific heat capacity | 900.0 - 963.0 J/(kg·K) Show Material materials with Specific heat capacity of 900.0 - 963.0 J/(kg·K) | Typical for Wrought 1000 Series Aluminium |
Thermal conductivity | 167.0 - 244.0 W/(m·K) Show Material materials with Thermal conductivity of 167.0 - 244.0 W/(m·K) | Typical for Wrought 1000 Series Aluminium |
Electrical
Property | Value | Comment |
---|---|---|
Electrical conductivity | 33000000.0 - 38000000.0 S/m Show Material materials with Electrical conductivity of 33000000.0 - 38000000.0 S/m | Typical for Wrought 1000 Series Aluminium |
Electrical resistivity | 2.7e-08 - 3e-08 Ω·m Show Material materials with Electrical resistivity of 2.7e-08 - 3e-08 Ω·m | Typical for Wrought 1000 Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminium | 99.0 % Show Material materials with Aluminium of 99.0 % | O | ASTM B211 | Bar, Rod, Wire |
Copper | 0.05 - 0.2 % Show Material materials with Copper of 0.05 - 0.2 % | O | ASTM B211 | Bar, Rod, Wire |
Manganese | 0.05 Show Material materials with Manganese of 0.05 | O | ASTM B211 | Bar, Rod, Wire |
Zinc | 0.1 Show Material materials with Zinc of 0.1 | O | ASTM B211 | Bar, Rod, Wire |
Technological properties
Property | ||
---|---|---|
Brazing | Excellent | |
Workability | Excellent workability. |