EN 573-3 Grade AW-2117 T4

Want to keep this datasheet? Save it now in your required format

Description

Age-hardenable AlCu alloy. The alloy is not food safe.

Related Standards

Equivalent Materials

This material data has been provided by WIAM,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueConditionRelated StandardsShape

Density

2.75 g/cm³

Show Material materials with Density of 2.75 g/cm³

T4

EN 573-3, EN 1301

Wire

20.0 °C

2.74 g/cm³

Show Material materials with Density of 2.74 g/cm³

T4

EN 573-3

Wire

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Elastic modulus

70.0 GPa

Show Material materials with Elastic modulus of 70.0 GPa

T4

EN 573-3, EN 1301

Wire

20.0 °C

67.0 GPa

Show Material materials with Elastic modulus of 67.0 GPa

T4

EN 573-3

Wire

Elongation

20.0 %

Show Material materials with Elongation of 20.0 %

T4

EN 573-3, EN 1301

Wire

20.0 °C

5.0 %

Show Material materials with Elongation of 5.0 %

T4

EN 573-3

Wire

A100

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 2000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 2000 Series Aluminium

Shear modulus

20.0 °C

25.5 GPa

Show Material materials with Shear modulus of 25.5 GPa

T4

EN 573-3

Wire

Tensile strength

260.0 MPa

Show Material materials with Tensile strength of 260.0 MPa

T4

EN 573-3, EN 1301

Wire

20.0 °C

170.0 - 240.0 MPa

Show Material materials with Tensile strength of 170.0 - 240.0 MPa

T4

EN 573-3

Wire

Thermal

PropertyTemperatureValueConditionRelated StandardsShape

Coefficient of thermal expansion

-50.0 °C

2.18e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.18e-05 1/K

T4

EN 573-3

Wire

20 °C

2.38e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.38e-05 1/K

T4

EN 573-3, EN 1301

Wire

100.0 °C

2.34e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.34e-05 1/K

T4

EN 573-3

Wire

100 °C

2.38e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.38e-05 1/K

T4

EN 573-3, EN 1301

Wire

200.0 °C

2.45e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.45e-05 1/K

T4

EN 573-3

Wire

300.0 °C

2.56e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.56e-05 1/K

T4

EN 573-3

Wire

Melting point

550.0 - 650.0 °C

Show Material materials with Melting point of 550.0 - 650.0 °C

T4

EN 573-3, EN 1301

Wire

Specific heat capacity

20.0 °C

898.0 J/(kg·K)

Show Material materials with Specific heat capacity of 898.0 J/(kg·K)

T4

EN 573-3

Wire

Thermal conductivity

155 W/(m·K)

Show Material materials with Thermal conductivity of 155 W/(m·K)

T4

EN 573-3, EN 1301

Wire

20.0 °C

150.0 - 180.0 W/(m·K)

Show Material materials with Thermal conductivity of 150.0 - 180.0 W/(m·K)

T4

EN 573-3

Wire

Electrical

PropertyTemperatureValueConditionRelated StandardsShape

Electrical conductivity

23000000.0 S/m

Show Material materials with Electrical conductivity of 23000000.0 S/m

T4

EN 573-3, EN 1301

Wire

20.0 °C

21000000.0 - 25000000.0 S/m

Show Material materials with Electrical conductivity of 21000000.0 - 25000000.0 S/m

T4

EN 573-3

Wire

Electrical resistivity

4.35e-08 Ω·m

Show Material materials with Electrical resistivity of 4.35e-08 Ω·m

T4

EN 573-3, EN 1301

Wire

Chemical properties

PropertyValueConditionRelated StandardsShape

Chromium

0.1 %

Show Material materials with Chromium of 0.1 %

T4

EN 573-3, EN 1301

Wire

Copper

2.2 - 3.0 %

Show Material materials with Copper of 2.2 - 3.0 %

T4

EN 573-3, EN 1301

Wire

Iron

0.7 %

Show Material materials with Iron of 0.7 %

T4

EN 573-3

Wire

0.70 %

Show Material materials with Iron of 0.70 %

T4

EN 573-3, EN 1301

Wire

Magnesium

0.2 - 0.5 %

Show Material materials with Magnesium of 0.2 - 0.5 %

T4

EN 573-3, EN 1301

Wire

Manganese

0.2 %

Show Material materials with Manganese of 0.2 %

T4

EN 573-3, EN 1301

Wire

Silicon

0.8 %

Show Material materials with Silicon of 0.8 %

T4

EN 573-3, EN 1301

Wire

Zinc

0.25 %

Show Material materials with Zinc of 0.25 %

T4

EN 573-3, EN 1301

Wire

Technological properties

Property
Brazing

hard brazing (with flux/ without flux): sufficient / sufficient

Corrosion properties

Seawater: poor, weathering: poor

Workability

Moderate Workability