JIS H4000 Grade 5052 hot-rolled

Want to keep this datasheet? Save it now in your required format

Description

Aluminum JIS 5052 is a non-heat treatable alloy with excellent finishing qualities. JIS 5052 offers better corrosion resistance than most aluminum alloys, especially to salt water and marine atmospheres. This alloy can be readily welded using most common techniques and is in fact offers some of the best welding characteristics of all aluminum alloys.

Related Standards

Equivalent Materials

This material data has been provided by Japanese Industrial Standards.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueComment

Density

2.65 - 2.7 g/cm³

Show Material materials with Density of 2.65 - 2.7 g/cm³

Typical for Wrought 5000 Series Aluminium

Mechanical

PropertyValueConditionRelated StandardsComment

Elastic modulus

69.0 - 70.0 GPa

Show Material materials with Elastic modulus of 69.0 - 70.0 GPa

Typical for Wrought 5000 Series Aluminium

Elongation

7.0 %

Show Material materials with Elongation of 7.0 %

hot-rolled

JIS H4000

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 5000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 5000 Series Aluminium

Shear modulus

26.0 - 26.5 GPa

Show Material materials with Shear modulus of 26.0 - 26.5 GPa

Typical for Wrought 5000 Series Aluminium

Tensile strength

196.0 MPa

Show Material materials with Tensile strength of 196.0 MPa

hot-rolled

JIS H4000

Yield strength

108.0 MPa

Show Material materials with Yield strength of 108.0 MPa

hot-rolled

JIS H4000

Thermal

PropertyValueComment

Coefficient of thermal expansion

2.2e-05 - 2.5e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.2e-05 - 2.5e-05 1/K

Typical for Wrought 5000 Series Aluminium

Max service temperature

150.0 °C

Show Material materials with Max service temperature of 150.0 °C

Typical for Wrought 5000 Series Aluminium

Melting point

560.0 - 655.0 °C

Show Material materials with Melting point of 560.0 - 655.0 °C

Typical for Wrought 5000 Series Aluminium

Specific heat capacity

879.0 - 963.0 J/(kg·K)

Show Material materials with Specific heat capacity of 879.0 - 963.0 J/(kg·K)

Typical for Wrought 5000 Series Aluminium

Thermal conductivity

112.0 - 205.0 W/(m·K)

Show Material materials with Thermal conductivity of 112.0 - 205.0 W/(m·K)

Typical for Wrought 5000 Series Aluminium

Electrical

PropertyValueComment

Electrical conductivity

18000000.0 - 31000000.0 S/m

Show Material materials with Electrical conductivity of 18000000.0 - 31000000.0 S/m

Typical for Wrought 5000 Series Aluminium

Electrical resistivity

3.3e-08 - 5e-08 Ω·m

Show Material materials with Electrical resistivity of 3.3e-08 - 5e-08 Ω·m

Typical for Wrought 5000 Series Aluminium

Technological properties

Property
Workability

Good workability.