JIS Z3263 Grade BA11PC H12

Want to keep this datasheet? Save it now in your required format

Description

Aluminum JIS BA11PC is a popular alloy that offers customers very good atmospheric corrosion resistance and moderate strength. Aluminum 3003 offers good machinability for aluminum alloys, though it is not heat treatable. Unlike other aluminum alloys, JIS BA11PC is weldable by conventional welding methods. It also takes cold and hot working well and has generally better mechanical properties when compared to 1000 series aluminum alloys.

Related Standards

Equivalent Materials

This material data has been provided by Japanese Industrial Standards.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueComment

Density

2.72 - 2.73 g/cm³

Show Material materials with Density of 2.72 - 2.73 g/cm³

Typical for Wrought 3000 Series Aluminium

Mechanical

PropertyValueConditionRelated StandardsComment

Elastic modulus

69.5 - 70.0 GPa

Show Material materials with Elastic modulus of 69.5 - 70.0 GPa

Typical for Wrought 3000 Series Aluminium

Elongation

2.0 %

Show Material materials with Elongation of 2.0 %

H12

JIS Z3263

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 3000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 3000 Series Aluminium

Shear modulus

25.0 - 26.0 GPa

Show Material materials with Shear modulus of 25.0 - 26.0 GPa

Typical for Wrought 3000 Series Aluminium

Tensile strength

118.0 MPa

Show Material materials with Tensile strength of 118.0 MPa

H12

JIS Z3263

Thermal

PropertyValueComment

Coefficient of thermal expansion

2.2e-05 - 2.4e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.2e-05 - 2.4e-05 1/K

Typical for Wrought 3000 Series Aluminium

Melting point

629.0 - 654.0 °C

Show Material materials with Melting point of 629.0 - 654.0 °C

Typical for Wrought 3000 Series Aluminium

Specific heat capacity

893.0 - 920.0 J/(kg·K)

Show Material materials with Specific heat capacity of 893.0 - 920.0 J/(kg·K)

Typical for Wrought 3000 Series Aluminium

Thermal conductivity

154.0 - 193.0 W/(m·K)

Show Material materials with Thermal conductivity of 154.0 - 193.0 W/(m·K)

Typical for Wrought 3000 Series Aluminium

Electrical

PropertyValueComment

Electrical conductivity

23000000.0 - 29000000.0 S/m

Show Material materials with Electrical conductivity of 23000000.0 - 29000000.0 S/m

Typical for Wrought 3000 Series Aluminium

Electrical resistivity

3.4e-08 - 4.2e-08 Ω·m

Show Material materials with Electrical resistivity of 3.4e-08 - 4.2e-08 Ω·m

Typical for Wrought 3000 Series Aluminium

Technological properties

Property
Processing history

H12

Workability

Good workability.