General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 2.72 - 2.8 g/cm³ Show Material materials with Density of 2.72 - 2.8 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 69 GPa Show Material materials with Elastic modulus of 69 GPa | |
Elongation | 23.0 °C | 4.5 - 7 % Show Material materials with Elongation of 4.5 - 7 % | |
Elongation A50 | 23.0 °C | 1 - 7 % Show Material materials with Elongation A50 of 1 - 7 % | |
Plane-Strain Fracture Toughnes | 23.0 °C | 22 - 35 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22 - 35 MPa·√m | Typical for Wrought 3000 Series Aluminium |
Poisson's ratio | 23.0 °C | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Wrought 3000 Series Aluminium |
Shear modulus | 23.0 °C | 25 GPa Show Material materials with Shear modulus of 25 GPa | |
Shear strength | 23.0 °C | 97 MPa Show Material materials with Shear strength of 97 MPa | |
Tensile strength | 23.0 °C | 130 - 180 MPa Show Material materials with Tensile strength of 130 - 180 MPa | |
Yield strength | 23.0 °C | 120 MPa Show Material materials with Yield strength of 120 MPa | |
Yield strength Rp0.2 | 23.0 °C | 105 - 130 MPa Show Material materials with Yield strength Rp0.2 of 105 - 130 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 20.0 °C | 2.36E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.36E-5 1/K |
23.0 °C | 2.4E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.4E-5 1/K | |
100.0 °C | 2.36E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.36E-5 1/K | |
Melting point | 635 - 655 °C Show Material materials with Melting point of 635 - 655 °C | |
Specific heat capacity | 23.0 °C | 900 J/(kg·K) Show Material materials with Specific heat capacity of 900 J/(kg·K) |
Thermal conductivity | 23.0 °C | 170 - 172 W/(m·K) Show Material materials with Thermal conductivity of 170 - 172 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 23.0 °C | 2.60E+7 S/m Show Material materials with Electrical conductivity of 2.60E+7 S/m |
Electrical resistivity | 23.0 °C | 3.85E-8 Ω·m Show Material materials with Electrical resistivity of 3.85E-8 Ω·m |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 96 - 99.5 % Show Material materials with Aluminium of 96 - 99.5 % | |
Chromium | 0 - 0.2 % Show Material materials with Chromium of 0 - 0.2 % | |
Copper | 0 - 0.3 % Show Material materials with Copper of 0 - 0.3 % | |
Iron | 0 - 0.7 % Show Material materials with Iron of 0 - 0.7 % | |
Magnesium | 0.2 - 0.8 % Show Material materials with Magnesium of 0.2 - 0.8 % | |
Manganese | 0.3 - 0.8 % Show Material materials with Manganese of 0.3 - 0.8 % | |
Other | 0 - 0.15 % Show Material materials with Other of 0 - 0.15 % | each 0.05, total 0.15, Rest Al |
Silicon | 0 - 0.6 % Show Material materials with Silicon of 0 - 0.6 % | |
Titanium | 0 - 0.1 % Show Material materials with Titanium of 0 - 0.1 % | |
Zinc | 0 - 0.4 % Show Material materials with Zinc of 0 - 0.4 % |
Technological properties
Property | ||
---|---|---|
Brazing | general: possible with commercial processes and methods | |
Corrosion properties | Stress corrosion cracking: no damage during operation and laboratory tests, general: very good, without protection in industrial or seawater atmosphere | |
General machinability | General: not suitable (O, H12), poor (H14, H25, H16, H18) | |
Workability | general (condition): good (O), acceptable (H12, H14, H25), poor(H16, H18) |