This website uses cookies to improve service quality. You will find more information about cookies on the privacy policy page.

Customize your search with filters

Contact suppliers of this material now

North America

Europe, UK

75 Lane Road, Fairfield, New Jersey 07004, United States

Europe, Europe, Belgium, Greece

Asia, North America, Europe

USA, North America

Unit 479 Ranglet Road, Walton Summit Centre, Bamber Bridge, Preston, Lancashire, PR5 8AR, United Kingdom, Europe

55 Winans Avenue, Cranford, New Jersey 07016, United States, North America

North America, Europe, Asia

Spain, Europe

3105-H28 Aluminium

.XLSX
.PDF
Save

Properties

Electrical

Electrical conductivity σel

2.55E+8 S/m at 20 °C

General

Density ρ

2.8 g/cm³ at 20 °C

Mechanical

Elastic modulus E

69 GPa at 20 °C

Elongation A

4.2 % at 20 °C

Tensile strength Rm

220 MPa at 20 °C

Yield strength YS

190 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

2.4E-5 1/K at 20 °C

Melting point Tm

640 °C

Specific heat capacity cp

900 J/(kg·K) at 20 °C

Thermal conductivity λ

170 W/(m·K) at 20 °C

Chemical properties

Element

Weight %

Comment

Al

96 - 99.5 %

Mn

0.3 - 0.8 %

Mg

0.2 - 0.8 %

Zn

0 - 0.4 %

Ti

0 - 0.1 %

More

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Contact suppliers of this material now

North America

Europe, UK

75 Lane Road, Fairfield, New Jersey 07004, United States

Europe, Europe, Belgium, Greece

Asia, North America, Europe

USA, North America

Unit 479 Ranglet Road, Walton Summit Centre, Bamber Bridge, Preston, Lancashire, PR5 8AR, United Kingdom, Europe

55 Winans Avenue, Cranford, New Jersey 07016, United States, North America

North America, Europe, Asia

Spain, Europe