AA 5049 H15

Want to keep this datasheet? Save it now in your required format

Description

Equivalent Materials

Ashby charts

See where AA 5049 H15 falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

2.7 g/cm³ at 23 °C

Mechanical

Elastic modulus

E

71 GPa at 23 °C

Show 5000 Series materials with Elastic modulus of 71 GPa at 23 °C

Elongation

A

3.5 % at 23 °C

Show 5000 Series materials with Elongation of 3.5 % at 23 °C

Plane-Strain Fracture Toughnes

KIC

22 - 35 MPa·√m at 23 °C

Show 5000 Series materials with Plane-Strain Fracture Toughnes of 22 - 35 MPa·√m at 23 °C

Typical for Wrought 5000 Series Aluminium

Poisson's ratio

ν

0.33 [-] at 23 °C

Show 5000 Series materials with Poisson's ratio of 0.33 [-] at 23 °C

Typical for Wrought 5000 Series Aluminium

Shear modulus

G

26 - 26.5 GPa at 23 °C

Show 5000 Series materials with Shear modulus of 26 - 26.5 GPa at 23 °C

Typical for Wrought 5000 Series Aluminium

Tensile strength

Rm

270 MPa at 23 °C

Show 5000 Series materials with Tensile strength of 270 MPa at 23 °C

Yield strength

YS

210 MPa at 23 °C

Show 5000 Series materials with Yield strength of 210 MPa at 23 °C

Thermal

Coefficient of thermal expansion

α

2.4E-5 1/K at 23 °C

Max service temperature

Tmax

150 °C

Typical for Wrought 5000 Series Aluminium

Melting point

Tm

620 °C

Specific heat capacity

cp

900 J/(kg·K) at 23 °C

Thermal conductivity

λ

140 W/(m·K) at 23 °C

Electrical

Electrical conductivity

σel

1.80E+7 - 3.10E+7 S/m at 23 °C

Typical for Wrought 5000 Series Aluminium

Electrical resistivity

ρel

3.3E-8 - 5E-8 Ω·m at 23 °C

Typical for Wrought 5000 Series Aluminium

Chemical properties

Element

Weight %

Comment

Al

94.7 - 97.9 %

Mg

1.6 - 2.5 %

Mn

0.5 - 1.1 %

Cr

0 - 0.3 %

Cu

0 - 0.1 %

More

Technological properties

Workability

Good workability.

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.