AA Standards Grade 5083 H321

Want to keep this datasheet? Save it now in your required format

Description

Aluminium 5083 is known for exceptional performance in extreme environments. 5083 is highly resistant to attack by both seawater and industrial chemical environments. Alloy 5083 also retains exceptional strength afterwelding. It has the highest strength of the non-heat treatable alloys but is not recommended for use in temperatures in excess of 65°C.

Related Standards

Equivalent Materials

This material data has been provided by AluKey,MakeItFrom.com,Righton Blackburns.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionRelated StandardsShape

Density

2.7 g/cm³

Show Material materials with Density of 2.7 g/cm³

H321

2.65 g/cm³

Show Material materials with Density of 2.65 g/cm³

H321

BS EN 573-3, BS EN 485-2

Plate, Sheet

Mechanical

PropertyValueConditionRelated StandardsShapeComment

Elastic modulus

71.0 GPa

Show Material materials with Elastic modulus of 71.0 GPa

H321

72.0 GPa

Show Material materials with Elastic modulus of 72.0 GPa

H321

BS EN 573-3, BS EN 485-2

Plate, Sheet

Elongation

12.0 %

Show Material materials with Elongation of 12.0 %

H321

AA Standards, ASTM B547

A50

13.0 %

Show Material materials with Elongation of 13.0 %

H321

Hardness, Vickers

95.0 [-]

Show Material materials with Hardness, Vickers of 95.0 [-]

H321

BS EN 573-3, BS EN 485-2

Plate, Sheet

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 5000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 5000 Series Aluminium

Shear modulus

26.0 - 26.5 GPa

Show Material materials with Shear modulus of 26.0 - 26.5 GPa

Typical for Wrought 5000 Series Aluminium

Shear strength

185.0 MPa

Show Material materials with Shear strength of 185.0 MPa

H321

BS EN 573-3, BS EN 485-2

Plate, Sheet

Tensile strength

305.0 - 385.0 MPa

Show Material materials with Tensile strength of 305.0 - 385.0 MPa

H321

AA Standards, ASTM B547

330.0 MPa

Show Material materials with Tensile strength of 330.0 MPa

H321

BS EN 573-3, BS EN 485-2

Plate, Sheet

Yield strength

215.0 MPa

Show Material materials with Yield strength of 215.0 MPa

H321

AA Standards, ASTM B547

RP02

240.0 MPa

Show Material materials with Yield strength of 240.0 MPa

H321

BS EN 573-3, BS EN 485-2

Plate, Sheet

RP02

240.0 MPa

Show Material materials with Yield strength of 240.0 MPa

H321

Thermal

PropertyValueConditionRelated StandardsShapeComment

Coefficient of thermal expansion

2.4e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.4e-05 1/K

H321

2.5e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.5e-05 1/K

H321

BS EN 573-3, BS EN 485-2

Plate, Sheet

Max service temperature

150.0 °C

Show Material materials with Max service temperature of 150.0 °C

Typical for Wrought 5000 Series Aluminium

Melting point

580.0 °C

Show Material materials with Melting point of 580.0 °C

H321

570.0 °C

Show Material materials with Melting point of 570.0 °C

H321

BS EN 573-3, BS EN 485-2

Plate, Sheet

Specific heat capacity

900.0 J/(kg·K)

Show Material materials with Specific heat capacity of 900.0 J/(kg·K)

H321

Thermal conductivity

120.0 W/(m·K)

Show Material materials with Thermal conductivity of 120.0 W/(m·K)

H321

121.0 W/(m·K)

Show Material materials with Thermal conductivity of 121.0 W/(m·K)

H321

BS EN 573-3, BS EN 485-2

Plate, Sheet

Electrical

PropertyValueConditionRelated StandardsShapeComment

Electrical conductivity

18000000.0 - 31000000.0 S/m

Show Material materials with Electrical conductivity of 18000000.0 - 31000000.0 S/m

Typical for Wrought 5000 Series Aluminium

Electrical resistivity

5.8e-08 Ω·m

Show Material materials with Electrical resistivity of 5.8e-08 Ω·m

H321

BS EN 573-3, BS EN 485-2

Plate, Sheet

Chemical properties

PropertyValueConditionRelated StandardsShapeComment

Aluminium

92.4 - 95.6 %

Show Material materials with Aluminium of 92.4 - 95.6 %

H321

Chromium

0.05 - 0.25 %

Show Material materials with Chromium of 0.05 - 0.25 %

H321

AA Standards, ASTM B547, BS EN 573-3, BS EN 485-2

Plate, Sheet

Copper

0.1 %

Show Material materials with Copper of 0.1 %

H321

AA Standards, ASTM B547, BS EN 573-3, BS EN 485-2

Plate, Sheet

Iron

0.40 %

Show Material materials with Iron of 0.40 %

H321

AA Standards, ASTM B547

0.4 %

Show Material materials with Iron of 0.4 %

H321

BS EN 573-3, BS EN 485-2

Plate, Sheet

Magnesium

4.0 - 4.9 %

Show Material materials with Magnesium of 4.0 - 4.9 %

H321

AA Standards, ASTM B547, BS EN 573-3, BS EN 485-2

Plate, Sheet

Manganese

0.4 - 1.0 %

Show Material materials with Manganese of 0.4 - 1.0 %

H321

AA Standards, ASTM B547, BS EN 573-3, BS EN 485-2

Plate, Sheet

Other

0.15 %

Show Material materials with Other of 0.15 %

H321

BS EN 573-3, BS EN 485-2

Plate, Sheet

Total

Silicon

0.4 %

Show Material materials with Silicon of 0.4 %

H321

AA Standards, ASTM B547, BS EN 573-3, BS EN 485-2

Plate, Sheet

Titanium

0.15 %

Show Material materials with Titanium of 0.15 %

H321

AA Standards, ASTM B547, BS EN 573-3, BS EN 485-2

Plate, Sheet

Zinc

0.25 %

Show Material materials with Zinc of 0.25 %

H321

AA Standards, ASTM B547, BS EN 573-3, BS EN 485-2

Plate, Sheet

Technological properties

Property
Application areas

Ship building, Rail cars, Vehicle bodies, Tip truck bodies, Mine skips and cages, Pressure vessels

Brazing

general: no brazing is known or developed

Corrosion properties

Stress corrosion cracking: kein Schadensfall im Betrieb und bei Labortests (O, H321, H116), kein Schadensfall im Betrieb, eingeschränkte Schäden bei den Labortests (H111), general: very good, without protection in industrial or seawater atmosphere

General machinability

General: poor

Workability

general (condition): acceptable (O), poor(H321, H116, H111)