Properties

General

Density

ρ

2.66 - 2.7 g/cm³ at 23 °C

Mechanical

Elastic modulus

E

71 GPa at 23 °C

Show 5000 Series materials with Elastic modulus of 71 GPa at 23 °C

Elongation

A

11 % at 23 °C

Show 5000 Series materials with Elongation of 11 % at 23 °C

Elongation A50

A50

12 % at 23 °C

Show 5000 Series materials with Elongation A50 of 12 % at 23 °C

Plane-Strain Fracture Toughnes

KIC

22 - 35 MPa·√m at 23 °C

Show 5000 Series materials with Plane-Strain Fracture Toughnes of 22 - 35 MPa·√m at 23 °C

Typical for Wrought 5000 Series Aluminium

Poisson's ratio

ν

0.33 [-] at 23 °C

Show 5000 Series materials with Poisson's ratio of 0.33 [-] at 23 °C

Typical for Wrought 5000 Series Aluminium

Shear modulus

G

26 - 26.5 GPa at 23 °C

Show 5000 Series materials with Shear modulus of 26 - 26.5 GPa at 23 °C

Typical for Wrought 5000 Series Aluminium

Tensile strength

Rm

290 - 310 MPa at 23 °C

Show 5000 Series materials with Tensile strength of 290 - 310 MPa at 23 °C

Yield strength

YS

220 MPa at 23 °C

Show 5000 Series materials with Yield strength of 220 MPa at 23 °C

Yield strength Rp0.2

Rp0.2

205 MPa at 23 °C

Show 5000 Series materials with Yield strength Rp0.2 of 205 MPa at 23 °C

Thermal

Coefficient of thermal expansion

α

2.38E-5 1/K at 20 °C

Hide chart

Max service temperature

Tmax

150 °C

Typical for Wrought 5000 Series Aluminium

Melting point

Tm

585 - 640 °C

Specific heat capacity

cp

900 J/(kg·K) at 23 °C

Thermal conductivity

λ

126 - 130 W/(m·K) at 23 °C

Electrical

Electrical conductivity

σel

1.80E+7 S/m at 23 °C

Electrical resistivity

ρel

5.56E-8 Ω·m at 23 °C

Chemical properties

Element

Weight %

Comment

Al

93 - 96.3 %

Mg

3.5 - 4.5 %

Mn

0.2 - 0.7 %

Cr

0.05 - 0.25 %

Cu

0 - 0.1 %

More

Technological properties

Brazing

general: no brazing is known or developed

Corrosion properties

Stress corrosion cracking: no damage during operation and laboratory tests (O, H32, H116, H111), no damage during operation, limited damage during laboratory tests (H34, H36, H38), general: very good, without protection in industrial or seawater atmosphere

General machinability

General: poor (O, H32, H116, H111), sufficient (H34, H36, H38)

Workability

general (condition): good (O), acceptable (H32, H116, H111), poor(H36, H38)

This material data has been provided by MakeItFrom.com,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.