See where AA 1050 H14 falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ2.7 g/cm³ at 20 °C
Coefficient of thermal expansion
α2.4E-5 1/K at 20 °C
Melting point
Tm650 °C
Specific heat capacity
cp900 J/(kg·K) at 20 °C
Thermal conductivity
λ230 W/(m·K) at 20 °C
Electrical conductivity
σel3.54E+8 S/m at 20 °C
Electrical resistivity
ρel2.7E-8 - 3E-8 Ω·m at 20 °C
Typical for Wrought 1000 Series Aluminium
Element
Weight %
Comment
99.5 - 100 %
0 - 0.05 %
0 - 0.4 %
0 - 0.05 %
0 - 0.05 %
Brazing
Excellent
Workability
Excellent workability.