AA Standards Grade 5154 H22

Want to keep this datasheet? Save it now in your required format

Description

Related Standards

Equivalent Materials

Ashby charts

See where AA Standards Grade 5154 H22 falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

2.66 - 2.7 g/cm³ at 23 °C

Dimension

Dimensions

Dicke

Mechanical

Elastic modulus

E

70 GPa at 23 °C

Show 5000 Series materials with Elastic modulus of 70 GPa at 23 °C

Elongation

A

5.8 % at 23 °C

Show 5000 Series materials with Elongation of 5.8 % at 23 °C

Elongation A100

A100

10 % at 23 °C

Show 5000 Series materials with Elongation A100 of 10 % at 23 °C

Elongation A50

A50

5 - 12 % at 23 °C

Show 5000 Series materials with Elongation A50 of 5 - 12 % at 23 °C

Plane-Strain Fracture Toughnes

KIC

22 - 35 MPa·√m at 23 °C

Show 5000 Series materials with Plane-Strain Fracture Toughnes of 22 - 35 MPa·√m at 23 °C

Typical for Wrought 5000 Series Aluminium

Poisson's ratio

ν

0.33 [-] at 23 °C

Show 5000 Series materials with Poisson's ratio of 0.33 [-] at 23 °C

Typical for Wrought 5000 Series Aluminium

Shear modulus

G

26 - 26.5 GPa at 23 °C

Show 5000 Series materials with Shear modulus of 26 - 26.5 GPa at 23 °C

Typical for Wrought 5000 Series Aluminium

Tensile strength

Rm

250 - 300 MPa at 23 °C

Show 5000 Series materials with Tensile strength of 250 - 300 MPa at 23 °C

Yield strength

YS

200 MPa at 23 °C

Show 5000 Series materials with Yield strength of 200 MPa at 23 °C

Yield strength Rp0.2

Rp0.2

180 MPa at 23 °C

Show 5000 Series materials with Yield strength Rp0.2 of 180 MPa at 23 °C

Thermal

Coefficient of thermal expansion

α

2.39E-5 1/K at 20 °C

Hide chart

Max service temperature

Tmax

150 °C

Typical for Wrought 5000 Series Aluminium

Melting point

Tm

590 - 645 °C

Specific heat capacity

cp

900 J/(kg·K) at 23 °C

Thermal conductivity

λ

126 - 130 W/(m·K) at 23 °C

Electrical

Electrical conductivity

σel

1.90E+7 S/m at 23 °C

Electrical resistivity

ρel

5.26E-8 Ω·m at 23 °C

Chemical properties

Element

Weight %

Comment

Al

94.4 - 96.8 %

Mg

3.1 - 3.9 %

Cr

0.15 - 0.35 %

Cu

0 - 0.1 %

Fe

0 - 0.4 %

More

Technological properties

Brazing

general: no brazing is known or developed

Corrosion properties

Stress corrosion cracking: no damage during operation and laboratory tests, general: very good, without protection in industrial or seawater atmosphere

General machinability

General: poor (O, H32), sufficient (H34, H36, H38)

Workability

general (condition): good (O), acceptable (H32, H34), poor(H36, H38)

This material data has been provided by MakeItFrom.com,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.