General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 2.7 g/cm³ Show Material materials with Density of 2.7 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 20.0 °C | 70 GPa Show Material materials with Elastic modulus of 70 GPa |
Elongation | 20.0 °C | 12 % Show Material materials with Elongation of 12 % |
Elongation A50 | 20.0 °C | 5 - 15 % Show Material materials with Elongation A50 of 5 - 15 % |
Hardness, Brinell | 20.0 °C | 67 [-] Show Material materials with Hardness, Brinell of 67 [-] |
Tensile strength | 20.0 °C | 250 - 270 MPa Show Material materials with Tensile strength of 250 - 270 MPa |
Yield strength | 20.0 °C | 200 MPa Show Material materials with Yield strength of 200 MPa |
Yield strength Rp0.2 | 20.0 °C | 180 - 205 MPa Show Material materials with Yield strength Rp0.2 of 180 - 205 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 20.0 °C | 2.4E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.4E-5 1/K |
Melting point | 590 °C Show Material materials with Melting point of 590 °C | |
Specific heat capacity | 20.0 °C | 900 J/(kg·K) Show Material materials with Specific heat capacity of 900 J/(kg·K) |
Thermal conductivity | 20.0 °C | 130 W/(m·K) Show Material materials with Thermal conductivity of 130 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Aluminium | 94.4 - 96.8 % Show Material materials with Aluminium of 94.4 - 96.8 % |
Chromium | 0.15 - 0.35 % Show Material materials with Chromium of 0.15 - 0.35 % |
Copper | 0.1 % Show Material materials with Copper of 0.1 % |
Iron | 0.4 % Show Material materials with Iron of 0.4 % |
Magnesium | 3.1 - 3.9 % Show Material materials with Magnesium of 3.1 - 3.9 % |
Manganese | 0.1 % Show Material materials with Manganese of 0.1 % |
Other | 0.15 % Show Material materials with Other of 0.15 % |
Silicon | 0.25 % Show Material materials with Silicon of 0.25 % |
Titanium | 0.2 % Show Material materials with Titanium of 0.2 % |
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % |