General
Property | Temperature | Value |
---|---|---|
Density | 20.0 °C | 2.7 g/cm³ Show Material materials with Density of 2.7 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 20.0 °C | 69 GPa Show Material materials with Elastic modulus of 69 GPa |
Elongation | 20.0 °C | 11 % Show Material materials with Elongation of 11 % |
Elongation A50 | 20.0 °C | 8 - 12 % Show Material materials with Elongation A50 of 8 - 12 % |
Hardness, Brinell | 20.0 °C | 73 [-] Show Material materials with Hardness, Brinell of 73 [-] |
Tensile strength | 20.0 °C | 205 - 250 MPa Show Material materials with Tensile strength of 205 - 250 MPa |
Yield strength | 20.0 °C | 210 MPa Show Material materials with Yield strength of 210 MPa |
Yield strength Rp0.2 | 20.0 °C | 170 - 215 MPa Show Material materials with Yield strength Rp0.2 of 170 - 215 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 20.0 °C | 2.3E-5 1/K Show Material materials with Coefficient of thermal expansion of 2.3E-5 1/K |
Melting point | 620 °C Show Material materials with Melting point of 620 °C | |
Specific heat capacity | 20.0 °C | 900 J/(kg·K) Show Material materials with Specific heat capacity of 900 J/(kg·K) |
Thermal conductivity | 20.0 °C | 200 W/(m·K) Show Material materials with Thermal conductivity of 200 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Aluminium | 97.5 - 99.4 % Show Material materials with Aluminium of 97.5 - 99.4 % |
Chromium | 0.1 % Show Material materials with Chromium of 0.1 % |
Copper | 0.1 % Show Material materials with Copper of 0.1 % |
Iron | 0.35 % Show Material materials with Iron of 0.35 % |
Magnesium | 0.45 - 0.9 % Show Material materials with Magnesium of 0.45 - 0.9 % |
Manganese | 0.1 % Show Material materials with Manganese of 0.1 % |
Other | 0.15 % Show Material materials with Other of 0.15 % |
Silicon | 0.2 - 0.6 % Show Material materials with Silicon of 0.2 - 0.6 % |
Titanium | 0.1 % Show Material materials with Titanium of 0.1 % |
Zinc | 0.1 % Show Material materials with Zinc of 0.1 % |