See where AA Standards Grade 6063 T62 falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ2.7 g/cm³ at 23 °C
Dimensions
Wanddicke
Coefficient of thermal expansion
α2.34E-5 1/K at 20 °C
Melting point
Tm615 - 655 °C
Specific heat capacity
cp900 J/(kg·K) at 23 °C
Thermal conductivity
λ193 - 218 W/(m·K) at 23 °C
Electrical conductivity
σel2.90E+7 - 3.40E+7 S/m at 23 °C
Electrical resistivity
ρel2.94E-8 - 3.45E-8 Ω·m at 23 °C
Element
Weight %
Comment
97.5 - 99.4 %
0.45 - 0.9 %
0.2 - 0.6 %
0 - 0.1 %
0 - 0.1 %
Brazing
general: possible with commercial processes and methods
Corrosion properties
Stress corrosion cracking: no damage during operation and laboratory tests, general: very good, without protection in industrial or seawater atmosphere
General machinability
General: poor (T1, T4), sufficient (T5, T452, T6, T83, T831, T832)
Workability
general (condition): acceptable (T1, T4, T5, T452), poor(T6, T83, T831, T832)
This material data has been provided by MakeItFrom.com,AluKey.