AA 6082 T6151

Want to keep this datasheet? Save it now in your required format

Equivalent Materials

This material data has been provided by MakeItFrom.com.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueCondition

Density

2.7 g/cm³

Show Material materials with Density of 2.7 g/cm³

T6151

Mechanical

PropertyValueConditionComment

Elastic modulus

72.0 GPa

Show Material materials with Elastic modulus of 72.0 GPa

T6151

Elongation

9.2 %

Show Material materials with Elongation of 9.2 %

T6151

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 6000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 6000 Series Aluminium

Shear modulus

26.0 - 26.5 GPa

Show Material materials with Shear modulus of 26.0 - 26.5 GPa

Typical for Wrought 6000 Series Aluminium

Tensile strength

320.0 MPa

Show Material materials with Tensile strength of 320.0 MPa

T6151

Yield strength

230.0 MPa

Show Material materials with Yield strength of 230.0 MPa

T6151

Thermal

PropertyValueConditionComment

Coefficient of thermal expansion

2.3e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.3e-05 1/K

T6151

Melting point

580.0 °C

Show Material materials with Melting point of 580.0 °C

T6151

Specific heat capacity

890.0 J/(kg·K)

Show Material materials with Specific heat capacity of 890.0 J/(kg·K)

T6151

Thermal conductivity

170.0 - 220.0 W/(m·K)

Show Material materials with Thermal conductivity of 170.0 - 220.0 W/(m·K)

Typical for Wrought 6000 Series Aluminium

Electrical

PropertyValueComment

Electrical conductivity

21000000.0 - 34000000.0 S/m

Show Material materials with Electrical conductivity of 21000000.0 - 34000000.0 S/m

Typical for Wrought 6000 Series Aluminium

Electrical resistivity

2.9e-08 - 5e-08 Ω·m

Show Material materials with Electrical resistivity of 2.9e-08 - 5e-08 Ω·m

Typical for Wrought 6000 Series Aluminium

Chemical properties

PropertyValueCondition

Aluminium

95.2 - 98.3 %

Show Material materials with Aluminium of 95.2 - 98.3 %

T6151

Chromium

0.25 %

Show Material materials with Chromium of 0.25 %

T6151

Copper

0.1 %

Show Material materials with Copper of 0.1 %

T6151

Iron

0.5 %

Show Material materials with Iron of 0.5 %

T6151

Magnesium

0.6 - 1.2 %

Show Material materials with Magnesium of 0.6 - 1.2 %

T6151

Manganese

0.4 - 1.0 %

Show Material materials with Manganese of 0.4 - 1.0 %

T6151

Other

0.15 %

Show Material materials with Other of 0.15 %

T6151

Silicon

0.7 - 1.3 %

Show Material materials with Silicon of 0.7 - 1.3 %

T6151

Titanium

0.1 %

Show Material materials with Titanium of 0.1 %

T6151

Zinc

0.2 %

Show Material materials with Zinc of 0.2 %

T6151

Technological properties

Property
Workability

Excellent workability.