AA 7005 O

Want to keep this datasheet? Save it now in your required format

Description

Equivalent Materials

Ashby charts

See where AA 7005 O falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

2.78 - 2.9 g/cm³ at 20 °C

Mechanical

Compressive modulus

Ecomp

72.4 MPa at 20 °C

Show 7000 Series materials with Compressive modulus of 72.4 MPa at 20 °C

Elastic modulus

E

71 GPa at 20 °C

Show 7000 Series materials with Elastic modulus of 71 GPa at 20 °C

Elongation

A

20 % at 20 °C

Show 7000 Series materials with Elongation of 20 % at 20 °C

Plane-Strain Fracture Toughnes

KIC

22 - 35 MPa·√m at 20 °C

Show 7000 Series materials with Plane-Strain Fracture Toughnes of 22 - 35 MPa·√m at 20 °C

Typical for Wrought 7000 Series Aluminium

Poisson's ratio

ν

0.33 [-] at 20 °C

Show 7000 Series materials with Poisson's ratio of 0.33 [-] at 20 °C

Typical for Wrought 7000 Series Aluminium

Shear modulus

G

26.9 GPa at 20 °C

Show 7000 Series materials with Shear modulus of 26.9 GPa at 20 °C

Shear strength

τ

117 MPa at 20 °C

Show 7000 Series materials with Shear strength of 117 MPa at 20 °C

Tensile strength

Rm

200 MPa at 20 °C

Show 7000 Series materials with Tensile strength of 200 MPa at 20 °C

Yield strength

YS

95 MPa at 20 °C

Show 7000 Series materials with Yield strength of 95 MPa at 20 °C

Thermal

Coefficient of thermal expansion

α

2.3E-5 1/K at 20 °C

Melting point

Tm

610 °C

Specific heat capacity

cp

880 J/(kg·K) at 20 °C

Thermal conductivity

λ

170 W/(m·K) at 20 °C

Electrical

Electrical conductivity

σel

2.50E+7 - 2.49E+8 S/m at 20 °C

Typical/derived value

Electrical resistivity

ρel

4.01E-8 Ω·m at 20 °C

Typical value

Specific Electrical conductivity

43 % IACS

Typical value

Chemical properties

Element

Weight %

Comment

Al

91 - 94.7 %

Zn

4 - 5 %

Mg

1 - 1.8 %

Mn

0.2 - 0.7 %

Zr

0.08 - 0.2 %

More

Technological properties

Brazing

Excellent

This material data has been provided by MakeItFrom.com,ASM Handbook Volume 2 Properties and Selection: Nonferrous Alloys and Special-Purpose Materials,WroughtAl_ElectricalResistivity.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.