See where AA 7005 T6 falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ2.78 - 2.9 g/cm³ at 20 °C
Coefficient of thermal expansion
α2.3E-5 1/K at 20 °C
Melting point
Tm610 °C
Specific heat capacity
cp880 J/(kg·K) at 20 °C
Thermal conductivity
λ137 - 140 W/(m·K) at 20 °C
unstated value
Electrical conductivity
σel2.03E+7 - 2.03E+8 S/m at 20 °C
Typical/derived value
Electrical resistivity
ρel2.9E-8 - 5.6E-8 Ω·m at 20 °C
Typical for Wrought 7000 Series Aluminium
Specific Electrical conductivity
35 % IACS
Typical value
Element
Weight %
Comment
91 - 94.7 %
4 - 5 %
1 - 1.8 %
0.2 - 0.7 %
0.08 - 0.2 %
Brazing
Excellent