Dimension

PropertyValue

Mechanical

PropertyValue

Chemical properties

Property

Carbon

1.2 - 1.35 %

Chromium

3.8 - 4.5 %

Copper

0.3 %

max.

Iron

Balance

Manganese

0.2 - 0.35 %

Molybdenum

0.7 - 1 %

Phosphorus

0.03 %

max.

Silicon

0.15 - 0.3 %

Sulfur

5E-3 %

max.

Tungsten

11.5 - 12.5 %

Vanadium

3.6 - 3.9 %

Technological properties

Property
Application areas

Mechanical engineering, industrial metrology, finishing and milling tools, cutting wheels, structural steels, reamers, turning and grooving steels for automatic work with good cooling

Processing history

Annealed