1.3401

Want to keep this datasheet? Save it now in your required format

Equivalent Materials

This material data has been provided by Remy Stahl.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Dimensions

Round-Bar length: 6-220 mm - Sheet: 20x15-100x10 mm - Rectangular Bar: 10-40 mm

Mechanical

PropertyValue

Hardness, Brinell

190.0 - 247.0 [-]

Show Supplier Material materials with Hardness, Brinell of 190.0 - 247.0 [-]

Tensile strength

1.0 - 800.0 MPa

Show Supplier Material materials with Tensile strength of 1.0 - 800.0 MPa

Chemical properties

PropertyValueComment

Carbon

1.1 - 1.3 %

Show Supplier Material materials with Carbon of 1.1 - 1.3 %

Manganese

12.0 - 13.0 %

Show Supplier Material materials with Manganese of 12.0 - 13.0 %

Phosphorus

1.0 %

Show Supplier Material materials with Phosphorus of 1.0 %

max.

Silicon

0.3 - 0.5 %

Show Supplier Material materials with Silicon of 0.3 - 0.5 %

Sulfur

0.04 %

Show Supplier Material materials with Sulfur of 0.04 %

max.

Technological properties

Property
Application areas

Wear-resistant components for grinding machines, such as crusher jaws, excavator bolts, excavator sleeves, gripping teeth and similarly stressed parts Safety engineering, grinding technology

Processing history

Solution Annealed