1.3817

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by Remy Stahl.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Dimensions

Round-Bar length: 42-100 mm

Mechanical

PropertyValue

Tensile strength

750.0 - 950.0 MPa

Show Supplier Material materials with Tensile strength of 750.0 - 950.0 MPa

Chemical properties

PropertyValueComment

Carbon

0.3 - 0.5 %

Show Supplier Material materials with Carbon of 0.3 - 0.5 %

Chromium

3.0 - 5.0 %

Show Supplier Material materials with Chromium of 3.0 - 5.0 %

Manganese

17.0 - 19.0 %

Show Supplier Material materials with Manganese of 17.0 - 19.0 %

Nickel

1 %

Show Supplier Material materials with Nickel of 1 %

max.

Nitrogen

0.1 %

Show Supplier Material materials with Nitrogen of 0.1 %

max.

Silicon

1 %

Show Supplier Material materials with Silicon of 1 %

max.

Sulfur

0.03 %

Show Supplier Material materials with Sulfur of 0.03 %

max.

Technological properties

Property
Application areas

Mechanical engineering, apparatus engineering, non-magnetisable components without special resistance to corrosion attacks

Processing history

Strain Hardened