1.3952

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by Remy Stahl.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Dimensions

Round-Bar length: 6-270 mm

Mechanical

PropertyValueComment

Elongation

35.0 - 40.0 %

Show Supplier Material materials with Elongation of 35.0 - 40.0 %

Hardness, Brinell

250 [-]

Show Supplier Material materials with Hardness, Brinell of 250 [-]

max.

Tensile strength

580.0 - 800.0 MPa

Show Supplier Material materials with Tensile strength of 580.0 - 800.0 MPa

Yield strength

280.0 MPa

Show Supplier Material materials with Yield strength of 280.0 MPa

min., RP02

Chemical properties

PropertyValueComment

Carbon

0.03 %

Show Supplier Material materials with Carbon of 0.03 %

max.

Chromium

16.5 - 18.5 %

Show Supplier Material materials with Chromium of 16.5 - 18.5 %

Manganese

2 %

Show Supplier Material materials with Manganese of 2 %

max.

Molybdenum

2.5 - 3.0 %

Show Supplier Material materials with Molybdenum of 2.5 - 3.0 %

Nickel

13.0 - 15.0 %

Show Supplier Material materials with Nickel of 13.0 - 15.0 %

Nitrogen

0.15 - 0.25 %

Show Supplier Material materials with Nitrogen of 0.15 - 0.25 %

Phosphorus

0.045 %

Show Supplier Material materials with Phosphorus of 0.045 %

max.

Silicon

1 %

Show Supplier Material materials with Silicon of 1 %

max.

Sulfur

0.015 %

Show Supplier Material materials with Sulfur of 0.015 %

max.

Technological properties

Property
Application areas

Metrology, mechanical engineering, connecting parts, shipbuilding

Corrosion properties

Resistant to intercrystalline corrosion, pitting and stress corrosion

Processing history

Solution Annealed