1.3964

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by Remy Stahl.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Mechanical

PropertyValue

Chemical properties

Property

Carbon

0.03 %

max.

Chromium

20 - 21.5 %

Iron

Balance

Manganese

4 - 6 %

Molybdenum

3 - 3.5 %

Nickel

15 - 17 %

Niobium

0.25 %

max.

Technological properties

Property
Application areas

Metrology, mechanical engineering, connecting parts, shipbuilding

Corrosion properties

Resistant to intercrystalline corrosion, pitting and stress corrosion

Processing history

Solution Annealed