Properties

Dimension

PropertyValue

Chemical properties

Property

Carbon

0.1 %

max.

Chromium

17 - 19 %

Iron

Balance

Manganese

7.5 - 9.5 %

Nickel

4.5 - 6.5 %

Nitrogen

0.1 - 0.2 %

Phosphorus

0.05 %

max.

Silicon

1 %

max.

Sulfur

0.03 %

max.

Technological properties

Property
Application areas

Mechanical engineering, connecting parts, components in shipbuilding and vehicle construction and for use in interior and exterior architecture and for pressure vessels down to -180 ° C

Processing history

Strain Hardened