1.4006

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by Remy Stahl.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Dimensions

Round-Bar length: 6 mm -50 mm

Mechanical

PropertyValueComment

Elongation

9 %

Show Supplier Material materials with Elongation of 9 %

min.

Tensile strength

650.0 - 850.0 MPa

Show Supplier Material materials with Tensile strength of 650.0 - 850.0 MPa

Yield strength

550.0 MPa

Show Supplier Material materials with Yield strength of 550.0 MPa

min., RP02

Chemical properties

PropertyValueComment

Carbon

0.08 - 0.15 %

Show Supplier Material materials with Carbon of 0.08 - 0.15 %

Chromium

11.5 - 13.5 %

Show Supplier Material materials with Chromium of 11.5 - 13.5 %

Manganese

1.5 %

Show Supplier Material materials with Manganese of 1.5 %

max.

Nickel

0.75 %

Show Supplier Material materials with Nickel of 0.75 %

max.

Phosphorus

0.04 %

Show Supplier Material materials with Phosphorus of 0.04 %

max.

Silicon

1 %

Show Supplier Material materials with Silicon of 1 %

max.

Sulfur

0.015 %

Show Supplier Material materials with Sulfur of 0.015 %

max.

Technological properties

Property
Application areas

Connecting parts, mechanical engineering, petrochemistry, hydraulic engineering, petroleum industry, construction parts in water and steam and mildly acting agents of the food industry as well as rifle barrels

Processing history

Quenched and Tempered