Properties

Dimension

PropertyValue

Mechanical

PropertyValue

Chemical properties

Property

Carbon

0.08 %

max.

Chromium

16 - 18 %

Iron

Balance

Manganese

1 %

max.

Phosphorus

0.04 %

max.

Silicon

1 %

max.

Sulfur

0.015 %

max.

Technological properties

Property
Application areas

Food technology, apparatus engineering, vehicle construction, plant engineering, parts for higher corrosion requirements with good deep-drawing and polishing properties, such as cutlery, sink linings, bumpers, wheel trims etc.

Processing history

Annealed