1.4120

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by Remy Stahl.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Dimensions

Round-Bar length: 16-52.15 mm

Mechanical

PropertyValueComment

Tensile strength

770 MPa

Show Supplier Material materials with Tensile strength of 770 MPa

max.

Chemical properties

PropertyValueComment

Carbon

0.17 - 0.22 %

Show Supplier Material materials with Carbon of 0.17 - 0.22 %

Chromium

12.0 - 14.0 %

Show Supplier Material materials with Chromium of 12.0 - 14.0 %

Manganese

1.0 %

Show Supplier Material materials with Manganese of 1.0 %

max.

Molybdenum

0.9 - 1.3 %

Show Supplier Material materials with Molybdenum of 0.9 - 1.3 %

Nickel

1.0 %

Show Supplier Material materials with Nickel of 1.0 %

max.

Phosphorus

0.04 %

Show Supplier Material materials with Phosphorus of 0.04 %

max.

Silicon

1.0 %

Show Supplier Material materials with Silicon of 1.0 %

max.

Sulfur

0.02 %

Show Supplier Material materials with Sulfur of 0.02 %

max.

Technological properties

Property
Application areas

Plant engineering, apparatus engineering, turbine blades, valve seats in superheated steam valves for temperatures up to approx. 500° C

Processing history

Quenched and Tempered