Properties

Dimension

PropertyValue

Dimensions

Round-Bar length: 5-340 mm

Chemical properties

PropertyValueComment

Carbon

0.95 - 1.2 %

Show Supplier Material materials with Carbon of 0.95 - 1.2 %

Chromium

0.4 - 0.8 %

Show Supplier Material materials with Chromium of 0.4 - 0.8 %

Manganese

1.0 %

Show Supplier Material materials with Manganese of 1.0 %

max.

Phosphorus

0.04 %

Show Supplier Material materials with Phosphorus of 0.04 %

max.

Silicon

1.0 %

Show Supplier Material materials with Silicon of 1.0 %

max.

Sulfur

0.04 %

Show Supplier Material materials with Sulfur of 0.04 %

max.

Technological properties

Property
Application areas

Apparatus engineering, shipbuilding, ultra-hardenable and wear-resistant steel, especially suitable for smaller stainless steel ball bearings

Processing history

Annealed