Properties

Dimension

PropertyValue

Dimensions

Round-Bar length: 16-165.10 mm

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

20 %

Show Supplier Material materials with Elongation of 20 %

min.

Hardness, Brinell

23.0 °C

310 [-]

Show Supplier Material materials with Hardness, Brinell of 310 [-]

max.

Tensile strength

23.0 °C

730 - 930 MPa

Show Supplier Material materials with Tensile strength of 730 - 930 MPa

Yield strength Rp0.2

23.0 °C

550 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 550 MPa

min.

Chemical properties

PropertyValueComment

Carbon

0.03 %

Show Supplier Material materials with Carbon of 0.03 %

max.

Chromium

24 - 26 %

Show Supplier Material materials with Chromium of 24 - 26 %

Iron

Balance

Manganese

2 %

Show Supplier Material materials with Manganese of 2 %

max.

Molybdenum

3 - 4.5 %

Show Supplier Material materials with Molybdenum of 3 - 4.5 %

Nickel

6 - 8 %

Show Supplier Material materials with Nickel of 6 - 8 %

Nitrogen

0.25 - 0.35 %

Show Supplier Material materials with Nitrogen of 0.25 - 0.35 %

Phosphorus

0.04 %

Show Supplier Material materials with Phosphorus of 0.04 %

max.

Silicon

1 %

Show Supplier Material materials with Silicon of 1 %

max.

Sulfur

0.015 %

Show Supplier Material materials with Sulfur of 0.015 %

max.

Technological properties

Property
Application areas

Plant construction, petrochemistry, apparatus engineering, chemistry, power plant construction, offshore, mechanical engineering, corrosion-resistant parts for the construction industry, mechanical engineering and general technical applications

Processing history

Solution Annealed