PropertyValue

Dimensions

Round-Bar length: 10-425 mm

Mechanical

PropertyValueComment

Elongation

14 %

Show Supplier Material materials with Elongation of 14 %

min.

Tensile strength

1.1 - 900.0 MPa

Show Supplier Material materials with Tensile strength of 1.1 - 900.0 MPa

Yield strength

700.0 MPa

Show Supplier Material materials with Yield strength of 700.0 MPa

min., RP02

Chemical properties

PropertyValueComment

Carbon

0.06 %

Show Supplier Material materials with Carbon of 0.06 %

max.

Chromium

15.0 - 17.0 %

Show Supplier Material materials with Chromium of 15.0 - 17.0 %

Manganese

1.5 %

Show Supplier Material materials with Manganese of 1.5 %

max.

Molybdenum

0.8 - 1.5 %

Show Supplier Material materials with Molybdenum of 0.8 - 1.5 %

Nickel

4.0 - 6.0 %

Show Supplier Material materials with Nickel of 4.0 - 6.0 %

Nitrogen

0.02 %

Show Supplier Material materials with Nitrogen of 0.02 %

max.

Phosphorus

0.04 %

Show Supplier Material materials with Phosphorus of 0.04 %

max.

Silicon

0.7 %

Show Supplier Material materials with Silicon of 0.7 %

max.

Sulfur

0.015 %

Show Supplier Material materials with Sulfur of 0.015 %

max.

Technological properties

Property
Application areas

Shipbuilding, offshore, plant construction, mechanical engineering, propeller shafts, axles, pump parts, centrifuge parts

Processing history

Quenched and Tempered