Dimension

PropertyValue

Dimensions

Round-Bar length: 12.7-165.1 mm

Mechanical

PropertyValueComment

Elongation

25 %

Show Supplier Material materials with Elongation of 25 %

min.

Hardness, Brinell

301 [-]

Show Supplier Material materials with Hardness, Brinell of 301 [-]

max.

Tensile strength

730.0 - 930.0 MPa

Show Supplier Material materials with Tensile strength of 730.0 - 930.0 MPa

Yield strength

550.0 MPa

Show Supplier Material materials with Yield strength of 550.0 MPa

min., RP02

Chemical properties

PropertyValueComment

Carbon

0.03 %

Show Supplier Material materials with Carbon of 0.03 %

max.

Chromium

24.0 - 26.0 %

Show Supplier Material materials with Chromium of 24.0 - 26.0 %

Copper

1.0 - 5.0 %

Show Supplier Material materials with Copper of 1.0 - 5.0 %

Manganese

1.0 %

Show Supplier Material materials with Manganese of 1.0 %

max.

Molybdenum

3.0 - 4.0 %

Show Supplier Material materials with Molybdenum of 3.0 - 4.0 %

Nickel

6.0 - 8.0 %

Show Supplier Material materials with Nickel of 6.0 - 8.0 %

Nitrogen

0.2 - 0.3 %

Show Supplier Material materials with Nitrogen of 0.2 - 0.3 %

Phosphorus

0.035 %

Show Supplier Material materials with Phosphorus of 0.035 %

max.

Silicon

1.0 %

Show Supplier Material materials with Silicon of 1.0 %

max.

Sulfur

0.015 %

Show Supplier Material materials with Sulfur of 0.015 %

max.

Tungsten

0.5 - 1.0 %

Show Supplier Material materials with Tungsten of 0.5 - 1.0 %

Technological properties

Property
Application areas

Plant construction, petrochemistry, apparatus engineering, chemistry, power plant construction, offshore, mechanical engineering

Processing history

Solution Annealed