1.4534.9

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by Remy Stahl.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Dimensions

Round-Bar length: 10-139.7 mm

Chemical properties

PropertyValueComment

Aluminium

0.8 - 1.35 %

Show Supplier Material materials with Aluminium of 0.8 - 1.35 %

Carbon

0.05 %

Show Supplier Material materials with Carbon of 0.05 %

max.

Chromium

12.25 - 13.25 %

Show Supplier Material materials with Chromium of 12.25 - 13.25 %

Manganese

0.1 %

Show Supplier Material materials with Manganese of 0.1 %

max.

Molybdenum

2.0 - 2.5 %

Show Supplier Material materials with Molybdenum of 2.0 - 2.5 %

Nickel

7.5 - 8.5 %

Show Supplier Material materials with Nickel of 7.5 - 8.5 %

Nitrogen

0.01 %

Show Supplier Material materials with Nitrogen of 0.01 %

max.

Phosphorus

0.01 %

Show Supplier Material materials with Phosphorus of 0.01 %

max.

Silicon

0.1 %

Show Supplier Material materials with Silicon of 0.1 %

max.

Sulfur

0.008 %

Show Supplier Material materials with Sulfur of 0.008 %

max.

Titanium

0.1 %

Show Supplier Material materials with Titanium of 0.1 %

max.

Technological properties

Property
Application areas

Vehicle construction, connecting parts, aerospace, mechanical engineering

Processing history

Solution Annealed