1.4539

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by Remy Stahl.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Dimensions

Round-Bar length: 24-150 mm - Hexagonal Bar: 17- 41 mm

Mechanical

PropertyValueComment

Elongation

35 %

Show Supplier Material materials with Elongation of 35 %

min.

Tensile strength

530.0 - 730.0 MPa

Show Supplier Material materials with Tensile strength of 530.0 - 730.0 MPa

Yield strength

220.0 MPa

Show Supplier Material materials with Yield strength of 220.0 MPa

min., RP02

Chemical properties

PropertyValueComment

Carbon

0.02 %

Show Supplier Material materials with Carbon of 0.02 %

max.

Chromium

19.0 - 21.0 %

Show Supplier Material materials with Chromium of 19.0 - 21.0 %

Copper

1.2 - 2.0 %

Show Supplier Material materials with Copper of 1.2 - 2.0 %

Manganese

2.0 %

Show Supplier Material materials with Manganese of 2.0 %

max.

Molybdenum

4.0 - 5.0 %

Show Supplier Material materials with Molybdenum of 4.0 - 5.0 %

Nickel

24.0 - 26.0 %

Show Supplier Material materials with Nickel of 24.0 - 26.0 %

Phosphorus

0.03 %

Show Supplier Material materials with Phosphorus of 0.03 %

max.

Silicon

0.7 %

Show Supplier Material materials with Silicon of 0.7 %

max.

Sulfur

0.01 %

Show Supplier Material materials with Sulfur of 0.01 %

max.

Technological properties

Property
Application areas

Plant engineering, petrochemistry, apparatus engineering, chemistry

Corrosion properties

Particularly good resistance to highly corrosive media such as phosphorus, sulphur and hydrochloric acid media

Processing history

Solution Annealed