1.4542 H1150D

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by Remy Stahl.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Dimensions

Round-Bar length: 5-370 mm partly ESU

Mechanical

PropertyValueComment

Elongation

16 %

Show Supplier Material materials with Elongation of 16 %

min.

Hardness, Brinell

311 [-]

Show Supplier Material materials with Hardness, Brinell of 311 [-]

min.

Tensile strength

860 MPa

Show Supplier Material materials with Tensile strength of 860 MPa

min.

Yield strength

725.0 MPa

Show Supplier Material materials with Yield strength of 725.0 MPa

min., RP02

Chemical properties

PropertyValueComment

Carbon

0.07 %

Show Supplier Material materials with Carbon of 0.07 %

max.

Chromium

15.0 - 17.0 %

Show Supplier Material materials with Chromium of 15.0 - 17.0 %

Copper

3.0 - 5.0 %

Show Supplier Material materials with Copper of 3.0 - 5.0 %

Manganese

1.5 %

Show Supplier Material materials with Manganese of 1.5 %

max.

Molybdenum

0.6 %

Show Supplier Material materials with Molybdenum of 0.6 %

max.

Nickel

3.0 - 5.0 %

Show Supplier Material materials with Nickel of 3.0 - 5.0 %

Phosphorus

0.04 %

Show Supplier Material materials with Phosphorus of 0.04 %

max.

Silicon

0.7 %

Show Supplier Material materials with Silicon of 0.7 %

max.

Sulfur

0.015 %

Show Supplier Material materials with Sulfur of 0.015 %

max.

Technological properties

Property
Application areas

Plant construction, mechanical engineering, medical technology, aerospace, screws and spindle material in valve construction, wheel and cover discs in compressor construction

Processing history

Hardened